| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil 101 Mobilgrease EAL
Mobilgrease EAL 101 and 102 are supreme performance greases designed specifically for applications which are environmentally sensitive. These products are biodegradable and virtually non-toxic greas..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil 221 Mobilgrease FM
Mobilgrease FM 221 and FM 222 are high performance multi-purpose products designed specifically for the lubrication of food processing machinery. Mobilgrease FM 221 and FM 222 are formulated with co..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil 222 Mobilgrease XHP Series
Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil 221 Mobilgrease XHP Series
Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil 223 Mobilgrease XHP Series
Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil Mobil Delvac Xtreme Service Grease
Mobil Delvac Xtreme Service Grease is an extra high performance extreme-pressure grease. It is an NLGI 2 grade and is manufactured with a proprietary, high-temperature lithium complex thickener syst..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil Mobilgrease 28
Mobilgrease 28 is a supreme performance, wide-temperature, antiwear grease designed to combine the unique features of a polyalphaolefin (PAO) synthetic base fluid with an organo-clay (non-soap) thic..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D-2509 |
|
ConocoPhillips Syncon® EP Heavy Duty Grease NLGI 1
Description: Conoco Syncon EP Heavy Duty Grease is an ultra high-performance synthetic base oil, lithium-complex grease specifically designed for extreme loading conditions. The combination of high-..
|
|||
| Four Ball Wear |
0.500
mm <br>@Temperature 75.0 °C,<br> Time 3600 sec
|
0.0197
in <br>@Temperature 167 °F,<br> Time 1.00 hour
|
1200 rpm, 40 kg, scar diameter; ASTM D2266, DIN 51 350/5 |
|
Chesterton 601 Chain Drive Pin & Bushing Lubricant
Description: Chesterton® 601 Chain Drive Pin & Bushing Lubricant is and has been the premium quality light lubricant of choice in industry for over thirty years. This superior lubricant was special..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | Scar Diameter |
|
ChevronTexaco Multifak® EP NLGI Grade 0
Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | Scar Diameter |
|
ChevronTexaco Multifak® EP NLGI Grade 2
Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | |
|
ChevronTexaco RPM® NLGI 1 Heavy Duty LC Grease EP
FeaturesChevron RPM Heavy Duty LC Greases EP are multipurpose, water resistant, extreme pressure, heavy duty chassis, wheel bearing, and general purpose lubricating greases.They are manufactured usi..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | Scar Diameter |
|
ChevronTexaco Starplex® Moly NLGI Grade 1
Texaco Starplex Moly greases deliver value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading — extending veh..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil 221 Mobilgrease XHP Series
Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil 222 Mobilgrease XHP Series
Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil 3 Mobilith AW Series
The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil 460 Mobilith SHC PM
Mobilith SHC PM greases are supreme performance products designed specifically for severe paper machine applications, including extreme temperature environments and exposure to different qualities o..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil CM-L Mobilgrease CM Series
Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil CM-P Mobilgrease CM Series
Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil CM-S Mobilgrease CM Series
Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil Mobilgrease HTS
Mobilgrease HTR, HTM, HTS and HTF are high performance Extreme Pressure greases with exceptional resistance to the water contamination conditions typical of steel mill, surface mining, and off-highw..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil Mobilith AW Series 00
The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | Scar Diameter; ASTM D4172 |
|
ConocoPhillips Hydroclear Diamond Class® 32 AW Turbine Oil
Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | Scar Diameter; ASTM D4172 |
|
ConocoPhillips Hydroclear Diamond Class® 46 AW Turbine Oil
Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | Scar Diameter |
|
ChevronTexaco Starplex® Moly NLGI Grade 2
Texaco Starplex Moly greases deliver value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading — extending veh..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | |
|
ConocoPhillips 1 Milube® Grease 2100T NLGI No. 1
Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic ..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D-2296 |
|
ConocoPhillips 595 NC Open Gear Lube
Description: Conoco Open Gear Lube 595 NC is a black, viscous, semi-fluid product that can be applied via central pumping systems that utilize injectors and nozzles for spray or drip application. Op..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil 461 Mobilgrease XHP Series
Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper..
|
|||
| Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
|
ExxonMobil Mobilgrease HTS
Mobilgrease HTR, HTM, HTS and HTF are high performance Extreme Pressure greases with exceptional resistance to the water contamination conditions typical of steel mill, surface mining, and off-highw..
|
|||
| Four Ball Wear |
0.500
mm <br>@Temperature 75.0 °C,<br> Time 3600 sec
|
0.0197
in <br>@Temperature 167 °F,<br> Time 1.00 hour
|
1200 rpm, 40 kg, scar diameter; ASTM D2266, DIN 51 350 |
|
Chesterton 652 Pneumatic Lubricant & Conditioner
Description: Chesterton® 652 Pneumatic Lubricant & Conditioner is a high performance, low viscosity, lubricating formula designed to creep into the internal workings of air tools, reduce wear and e..
|
|||