| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Four Ball Wear | 0.350 mm | 0.0138 in | 40 kg, 93°C, 600 rpm; ASTM D4172 |
|
ExxonMobil Mobil EAL 224H
Mobil EAL 224H is a premium performance environmentally aware hydraulic fluid designed to provide outstanding performance in hydraulic and circulation systems operating at moderate conditions. It pr..
|
|||
| Four Ball Wear |
0.350
mm <br>@Temperature 54.0 °C,<br> Time 3600 sec
|
0.0138
in <br>@Temperature 129 °F,<br> Time 1.00 hour
|
1800 rpm, 20 kg, scar diameter |
|
Chesterton 613 Moly Grease
Description: Chesterton® 613 Moly Grease is a high-performance, cost-effective lubricant that can withstand extreme temperatures and pressures for a wide range of high and low-speed applications. F..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | ASTM D4172 |
|
ELM® SoyLube® All Purpose Lubricant and Penetrating Oil
Description: SoyLube All Purpose Lubricant and Penetrating Oil is a high performance, biodegradable penetrant and lubricating oil for general purpose use. Formulated with the best optimized USA-gro..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | ASTM D2266 |
|
ExxonMobil Mobilgrease XTC
Mobilgrease XTC is an extra high performance product designed for use in high speed coupling applications. It is manufactured with a selected high viscosity mineral base oil and an extremely effecti..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | |
|
ConocoPhillips 220 Gear Oil AGMA Lubricant No. 5 EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | |
|
ConocoPhillips 320 Gear Oil AGMA Lubricant No. 6 EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | |
|
ConocoPhillips 460M Gear Oil AGMA Lubricant No.7EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172 |
|
ConocoPhillips ANDEROL® 6680 Synthetic Food Grade Gear Fluid
Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the ..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | 40 kg, 93°C, 600 rpm; ASTM D4172 |
|
ExxonMobil Mobil EAL 224H
Mobil EAL 224H is a premium performance environmentally aware hydraulic fluid designed to provide outstanding performance in hydraulic and circulation systems operating at moderate conditions. It pr..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | |
|
ConocoPhillips 100M Gear Oil AGMA Lubricant No. 3EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | |
|
ConocoPhillips 460 Gear Oil AGMA Lubricant No. 7 EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | |
|
ConocoPhillips 68 Gear Oil AGMA Lubricant No. 2 EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | |
|
ConocoPhillips 680 Gear Oil AGMA Lubricant No. 8EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | |
|
ConocoPhillips 1000 Gear Oil AGMA Lubricant No. 8AEP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | |
|
ConocoPhillips 150 Gear Oil AGMA Lubricant No. 4 EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | |
|
ConocoPhillips 100 Gear Oil AGMA Lubricant No. 3 EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | |
|
ConocoPhillips 220M Gear Oil AGMA Lubricant No. 5EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
|
|||
| Four Ball Wear | 0.350 mm | 0.0138 in | ASTM D2266 |
|
ExxonMobil Mobilgrease XTC
Mobilgrease XTC is an extra high performance product designed for use in high speed coupling applications. It is manufactured with a selected high viscosity mineral base oil and an extremely effecti..
|
|||