Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Four Ball Wear = 0.400 mm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Four Ball Wear 0.400 mm
0.0157 in
ASTM D2266
ExxonMobil 23 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Four Ball Wear 0.400 mm
0.0157 in
20 kg, 54°C, 1800 rpm, 1 hr; ASTM D4172
ExxonMobil Mobil Glygoyle 150
Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T..
Four Ball Wear 0.400 mm
0.0157 in
40 kg, 1200 rpm, 75°C, 1 hr
ExxonMobil Mobil Polyrex EP 2
Mobil Polyrex EP 2 is a shear-stable polyurea grease with excellent extreme-pressure (EP) and load-carrying characteristics. The proprietary polyurea thickener system exhibits excellent resistance t..
Four Ball Wear 0.400 mm
0.0157 in
Scar Diameter; ASTM D4172
ConocoPhillips Syncon® 220 Synthetic R&O Oil
Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv..
Four Ball Wear 0.400 mm
0.0157 in
Scar Diameter; ASTM D2266, DIN 51 350/5
Chesterton 615 High Temperature Grease
Description: Chesterton® 615 High Temperature Grease is the one grease to use for the most demanding of lubrication needs. It is a multi-purpose workhorse with outstanding extreme pressure capabili..
Four Ball Wear 0.400 mm
0.0157 in
ELM® TempFlex™ 35 to 160 w/ MoS2 Biodegradable Rail Curve Lubricant
Description: TempFlex™ 35 to 160 now with molybdenum disulphide is a premium quality biodegradable, Biotechbased™ Rail Curve Lubricant formulated from USA grown vegetable oils and a lithium-based ..
Four Ball Wear 0.400 mm
0.0157 in
Scar Diameter
ChevronTexaco Novatex® EP NLGI Grade 000
Texaco Novatex EP are water resistant, extreme pressure greases. They are manufactured using highly refined, select high viscosity index base oils, a calcium soap, and a specifically selected addit..
Four Ball Wear 0.400 mm
0.0157 in
Scar Diameter
ChevronTexaco PremiumRB
Texaco Premium RB delivers value through:Wide application range — Suitable for high rpm operation, operating temperatures ranging from -34°C to 177°C (-30°F to 350°F) and offers excellent rust ..
Four Ball Wear 0.400 mm
0.0157 in
ASTM D2266
ExxonMobil 111 Mobilux EP
Mobilux EP 111 is an extra high performance grease primarily designed for lubrication of all designs of couplings. It is specifically formulated to resist centrifugal separation of the oil from the ..
Four Ball Wear 0.400 mm
0.0157 in
ASTM D2266
ExxonMobil 3 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Four Ball Wear 0.400 mm
0.0157 in
ASTM D2266
ExxonMobil Mobil 1 Synthetic Grease
Mobil 1 Synthetic Grease is an NLGI No 2 high-performance grease which combines a synthetic base fluid with a lithium complex soap thickener. The thickener system provides a high dropping point, whi..
Four Ball Wear 0.400 mm
0.0157 in
1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172
ConocoPhillips ANDEROL® 6220 Synthetic Food Grade Gear Fluid
Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the ..
Four Ball Wear 0.400 mm
0.0157 in
1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172
ConocoPhillips ANDEROL® PQ AA 250 White Mineral Food Grade Gear Oil, ISO Grade 680, SAE Gear Oil Grade 250
Description: ANDEROL PQ AA Series Gear Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Gear..
Four Ball Wear 0.400 - 0.500 mm
0.0157 - 0.0197 in
Scar Diameter; ASTM D 2266
ConocoPhillips Gear Shield NC Open Gear Lubricant
Description: Conoco Gear Shield NC is a black, viscous fluid designed to lubricate open gears. Gear Shield NC contains neither chlorinated solvents nor lead compounds. Gear Shield NC is designed to ..
Four Ball Wear 0.400 mm
0.0157 in
ConocoPhillips Hydroclear® 1 Ultra-clean multi-purpose R&O Oil, AGMA Lubricant No. 1
Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks..
Four Ball Wear 0.400 mm
0.0157 in
ConocoPhillips Hydroclear® 220 Wet Gas Compressor Fluid ISO 220
Description: Conoco Hydroclear® Wet Gas Compressor Fluid is designed to lubricate rotary screw and reciprocating compressors in natural gas service. Conoco's high-quality, hydrocracked base oil..
Four Ball Wear 0.400 mm
0.0157 in
ConocoPhillips Hydroclear® 46 Multipurpose R&O Oil, AGMA Lubricant No. 1
Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidation inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear..
Four Ball Wear 0.400 mm
0.0157 in
ConocoPhillips Hydroclear® MV100 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
Four Ball Wear 0.400 mm

@Load 40.0 kg,
Temperature 150 °C
0.0157 in

@Load 88.2 lb,
Temperature 302 °F
mm<sup>2</sup>; 1800 RPM, 60 min; ASTM D4172
ConocoPhillips Synterra™ 2 Hydraulic Oil, AGMA No. 2
Description: Conoco Synterra Environmental Fluids Hydraulic and Circulating Oils give outstanding protection to equipment and the environment. These oils are made from synthetic polyol ester fluids ..
Four Ball Wear 0.400 mm

@Load 40.0 kg,
Temperature 150 °C
0.0157 in

@Load 88.2 lb,
Temperature 302 °F
mm<sup>2</sup>; 1800 RPM, 60 min; ASTM D4172
ConocoPhillips Synterra™ 3 Hydraulic Oil, AGMA No.3
Description: Conoco Synterra Environmental Fluids Hydraulic and Circulating Oils give outstanding protection to equipment and the environment. These oils are made from synthetic polyol ester fluids ..
Four Ball Wear 0.400 mm
0.0157 in
ASTM D2266
ExxonMobil 100 Mobiltemp SHC Series
Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base ..
Four Ball Wear 0.400 mm
0.0157 in
ASTM D2266
ExxonMobil 23 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Four Ball Wear 0.400 mm
0.0157 in
ConocoPhillips Hydroclear® 150 Gas Compressor Fluid
Description: Conoco Hydroclear Gas Compressor Fluid is designed to lubricate rotary screw and reciprocating compressors in natural gas service. Conoco's high-quality hydrocracked base oil, combi..
Four Ball Wear 0.400 mm
0.0157 in
ConocoPhillips Hydroclear® 320 Multipurpose R&O Oil, AGMA Lubricant No. 6
Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear ..
Four Ball Wear 0.400 mm
0.0157 in
ConocoPhillips Hydroclear® 46 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
Four Ball Wear 0.400 mm
0.0157 in
ASTM D2266
ExxonMobil 460 Special Mobiltemp SHC Series
Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base ..
Copyright © lookpolymers.com All Rights Reserved