Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature 23.0 °C
1.43 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycolac® INP630 ABS
INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance. Provides excellent hi..
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Geloy EXGY30CP ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Geloy XTWE480 ASA (Asia Pacific)
Anti-scratch Geloy grade with excellent weatherability, high flow, and good surface quality. XTWE480 is available in various colours.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East)
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East)
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180/1A
Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6
Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its ex..
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180/1A
Nilit Nilamid B G6 FR HF 30% Glass Fiber Reinforced, Flame Retardant PA6
Description: Nilamid B G6 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price..
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66 &nbsp;(Unverified Data**)
Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature 0.000 °C
1.43 ft-lb/in²
<br>@Temperature 32.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® 1760T PBT+PC (Europe-Africa-Middle East)
XENOY 1760T is developed as a easy flow material, for applications such as doorhandles and mirror housings. It is a 11% glass reinforced material with excellent strength and dimensional stability.Th..
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature 23.0 °C
1.43 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/1A
Sax Polymers SAXAMID 126K6 Nylon 6, 30% Glass Filled
SAXAMID 126K6 is a 30% glass beads filled polyamide 6 injection-molding-grade. It is characterized by dimensional stability, low warpage and good surface quality.Information provided by SAX Polymers..
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature 23.0 °C
1.43 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/1A
Sax Polymers SAXAMID 226K6 Nylon 6.6, 30% Glass Beads
SAXAMID 226K6 is a polyamide 6.6 injection-molding-grade filled with 30% glass beads. It is characterized by optimized shrinkage properties.Information provided by SAX Polymers
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature 23.0 °C
1.43 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A..
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Asia Pacific)
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A..
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
80x10x4; ISO 180/1A
Eurostar Staramide A28 PA66, Injection Molding
Staramide A28 is an Unreinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
80x10x4; ISO 180/1A
Eurostar Staramide A28K PA66, Heat Stabilized, Injection Molding
Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
80x10x4; ISO 180/1A
Eurostar Staramide A28N PA66, Nucleated, Injection Molding
Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -40.0 °C
1.43 ft-lb/in²
<br>@Temperature -40.0 °F
80x10x4; ISO 180/1A
Eurostar Staramide A28N PA66, Nucleated, Injection Molding
Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -40.0 °C
1.43 ft-lb/in²
<br>@Temperature -40.0 °F
80x10x4; ISO 180/1A
Eurostar Staramide B28H PA6, Heat Stabilized, Injection Molded
Staramide B28H is a Heat Stabilized, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -40.0 °C
1.43 ft-lb/in²
<br>@Temperature -40.0 °F
80x10x4; ISO 180/1A
Eurostar Staramide B28N PA6, Nucleated, Injection Molded
Staramide B28N is a Nucleated and Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -20.0 °C
1.43 ft-lb/in²
<br>@Temperature -4.00 °F
80x10x4; ISO 179/1eA
Eurostar Staramide RB006S PA66, 30% Glass Bead Filled, Injection Molded
Staramide RB006S is a 30% Glass Bead Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S3)Information provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -40.0 °C
1.43 ft-lb/in²
<br>@Temperature -40.0 °F
80x10x4; ISO 180/1A
Eurostar Starflam AF430B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR430B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -40.0 °C
1.43 ft-lb/in²
<br>@Temperature -40.0 °F
80x10x4; ISO 180/1A
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding
Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
80x10x4; ISO 180/1A
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding
Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -40.0 °C
1.43 ft-lb/in²
<br>@Temperature -40.0 °F
80x10x4; ISO 180/1A
Eurostar Starflam BFR552Y6 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR552Y6 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -40.0 °C
1.43 ft-lb/in²
<br>@Temperature -40.0 °F
80x10x4; ISO 180/1A
Eurostar Staramide ALY540A PA66, Glass/Mineral Fiber Reinforced, Injection Molding
Staramide ALY540A is a Glass Fiber Reinforced, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -40.0 °C
1.43 ft-lb/in²
<br>@Temperature -40.0 °F
80x10x4; ISO 180/1A
Eurostar Starflam B28UL PA6, Flame Retardant, Injection Molded
Starflam B28UL is Unfilled Halogen Free and Red Phosphorous Free, Flame Retardant, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180/1A
Eurotec® Tecolen® HP30 NL XC30 PPHP, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180/A
BASF Ultramid® C3U10 PA6/66 FR (Dry)
Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector..
Izod Impact, Notched (ISO) 3.00 kJ/m²
<br>@Temperature 23.0 °C
1.43 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/A
BASF Ultramid® C3U10 PA6/66 FR (Dry)
Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector..
Copyright © lookpolymers.com All Rights Reserved