Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 12.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East)
This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXD103 PC (Asia Pacific)
FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the ..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXD103 PC (Europe-Africa-Middle East)
FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the ..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXD951A PC
Visual effetcs diffusion, flame retardant PC with low/medium flow good for extrusion/injection molding applications. Ideal for light management platforms that require hiding power and transmission.T..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® FXC810SL PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810SL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require sparkle colour effects with lowered RFI inhibitor. Colour package may effect perform..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180/1A
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66
Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXD9945A PC (Europe-Africa-Middle East)
UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -40.0 °C
5.71 ft-lb/in²
<br>@Temperature -40.0 °F
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6 &nbsp;(Unverified Data**)
Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180-1A
Ineos ABS Lustran® Ultra 4115 ABS Pellets (a-methylstyrene-SAN / PC-modified), Very High Heat Grade
Lustran® Ultra 4115 is very high heat grade with high impact resistance and is PC-modified. It is used for the production of molded plastic articles.
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics PC1800 PC (Europe-Africa-Middle East)
PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold ..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics PC2200 PC (Asia Pacific)
PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East)
PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics PC6300 PC (Europe-Africa-Middle East)
PC6300 resin is a very high flow (MFR = 9.5 at 250ºC/1.2kg) polycarbonate product designed for use in the optical media market.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/1A
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber
SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -20.0 °C
5.71 ft-lb/in²
<br>@Temperature -4.00 °F
ISO 180/1A
Borealis EE002AE Polypropylene Elastomer Modified
EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180
Total PPC 9612 Polypropylene, Heterophasic Copolymer, Injection Molding
This product is a Total Ecosolutions grade.Polypropylene PPC 9612 has been developed specifically for the injection molding of crates and is characterized by a high Melt Flow index of 20 g/10 min. ..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Thickness 0.126 in,<br> Temperature -22.0 °F
complete break; b.o. ISO 180-A
Covestro Makrolon® 2258 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Thickness 0.126 in,<br> Temperature -22.0 °F
complete break; b.o. ISO 180-A
Covestro Makrolon® 2667 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Thickness 0.126 in,<br> Temperature -22.0 °F
complete break; b.o. ISO 180-A
Covestro Makrolon® FU1007 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecomid® NA40 GR30 NL RM PA 6.6 30% glass fiber reinforced, low friction and wear
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecomid® NA40 GR30 NL RT PA 6.6 30% glass fiber reinforced, very low friction and wear
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecomid® NA43 GR25 NL TD43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, high impact, heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
80x10x4; ISO 180/1A
Eurostar Staramide AG7 PA66, 35% Glass Filled, Injection Molded
AG7 is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180/1A
Eurotec® Tecomid® NA40 NL IX PA6.6, impact modified, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, Conditioned
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, Conditioned
Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -40.0 °C
5.71 ft-lb/in²
<br>@Temperature -40.0 °F
ISO 180
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, Conditioned
Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties ..
Copyright © lookpolymers.com All Rights Reserved