| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -30.0 °C |
1.43
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® G151 ABS (Europe-Africa-Middle East)
CYCOLAC G151 is a flame retardant grade of ´new technology´ CYCOLAC which has been especially formulated to minimise many of the problems often associated with the processing of traditiona..
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Thickness 4.00 mm, Temperature -20.0 °C |
1.43
ft-lb/in² @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
|
Premix Thermoplastics PRE-ELEC® PP 1399 Dissipative Thermoplastic Compound
PRE-ELEC® PP 1399 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resi..
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -30.0 °C |
1.43
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Geloy FXTW30PE ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -30.0 °C |
1.43
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Geloy XTWE480 ASA (Asia Pacific)
Anti-scratch Geloy grade with excellent weatherability, high flow, and good surface quality. XTWE480 is available in various colours.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -30.0 °C |
1.43
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific)
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -30.0 °C |
1.43
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East)
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -30.0 °C |
1.43
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer
Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health..
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -30.0 °C |
1.43
ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
|
Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6
Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its ex..
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature 23.0 °C |
1.43
ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
|
Sax Polymers SAXAMID 226K6 Nylon 6.6, 30% Glass Beads
SAXAMID 226K6 is a polyamide 6.6 injection-molding-grade filled with 30% glass beads. It is characterized by optimized shrinkage properties.Information provided by SAX Polymers
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -30.0 °C |
1.43
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl PKN4717 PPE+HIPS (Europe-Africa-Middle East)
NORYL PKN4717 is a PPO+PS concentrate for dilution with polystyrene resin for foam extrusion. It is suitable for (microwavable) food packaging and is compliant with US and European food contact regu..
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -30.0 °C |
1.43
ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
|
Styrolution Terblend® N NG-02 UV ABS / PA, 8% Glass filled
Terblend N NG-02 UV is an 8% glass fiber reinforced (UV stabilized) ABS/PA blend with enhanced dimensional stability and rigidity.High dimensional stabilityEnhanced rigidityEnhanced softening temper..
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -30.0 °C |
1.43
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature 23.0 °C |
1.43
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature 23.0 °C |
1.43
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Asia Pacific)
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -20.0 °C |
1.43
ft-lb/in² @Temperature -4.00 °F |
ISO 180/1A |
|
Domo 2340P Polypropylene Copolymer
Information provided by Domo.
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -40.0 °C |
1.43
ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
|
Eurostar Staramide A28K PA66, Heat Stabilized, Injection Molding
Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -40.0 °C |
1.43
ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
|
Eurostar Staramide AS10 PA66, 50% Glass Bead Reinforced, Injection Molding
Staramide AS10 is a 50% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -40.0 °C |
1.43
ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
|
Eurostar Staramide B28 PA6, Injection Molded
Staramide B28 is an Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -30.0 °C |
1.43
ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1A |
|
Eurostar Starflam AFR200Y PA66, Flame Retardant, Injection Molding
Staramide AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -40.0 °C |
1.43
ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
|
Eurostar Starflam AFR200Y PA66, Flame Retardant, Injection Molding
Staramide AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -40.0 °C |
1.43
ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
|
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding
Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -20.0 °C |
1.43
ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
|
Eurostar Starflam BFR552Y3 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR552Y3 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -40.0 °C |
1.43
ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
|
Eurostar Starflam BFR552Y3 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR552Y3 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -20.0 °C |
1.43
ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
|
Eurostar Starflam BFR552Y6 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR552Y6 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -30.0 °C |
1.43
ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
|
Eurotec® Tecodur® PB70 GB20 NL PBT, 20% glass bead reinforced, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -30.0 °C |
1.43
ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
|
Eurotec® Tecomid® NT40 NL XA60 PPA, unfilled, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature 23.0 °C |
1.43
ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
|
BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Dry)
Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector..
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -30.0 °C |
1.43
ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
|
BASF Ultramid® FRee B3U31G4 20% Glass Filled PA66 FR (Dry)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -40.0 °C |
1.43
ft-lb/in² @Temperature -40.0 °F |
ISO 180/4A |
|
Polykemi AB POLYfill PPH T5040 FC Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Izod Impact, Notched (ISO) |
3.00
kJ/m² @Temperature -40.0 °C |
1.43
ft-lb/in² @Temperature -40.0 °F |
ISO 180/4A |
|
Polykemi AB POLYfill PPH T5040 FC VT Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||