Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 30.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/1A
Nilit Nilamid B3 H ZC Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Europe-Africa-Middle East)
Improved flow PC with excellent processability and mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® 910A PC (Europe-Africa-Middle East)
LEXAN 910A is a low viscosity flame retardant grade, intended for electrical applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® FXD103 PC (Europe-Africa-Middle East)
FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the ..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXD124R PC (Europe-Africa-Middle East)
LEXAN FXD124R is a transparent/translucent low viscosity grade for light diffusion special effects. FDA compliant. Color package may affect performance.This data was supplied by SABIC-IP for the Eu..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Asia Pacific)
Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may ..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXD911A PC (Europe-Africa-Middle East)
Lexan FXD911A is a flame retardant, medium viscosity grade with release for the special effect appearance Diffusion in various colors. Color package may affect performance.This data was supplied by ..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Europe-Africa-Middle East)
Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer (Europe-Africa-Middle East)
Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HPM1944 PC (Asia Pacific)
Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). ..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Europe-Africa-Middle East)
Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® IR2840 PC
7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant, natural only.Effective January 15th, 2007 this grade will no longer be supported with biocompatibilit..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle ..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer
Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer (Asia Pacific)
Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® C CM 406 U Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics PC2200R PC (Asia Pacific)
PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics PC2203R PC
PC2203R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/A
Styrolution Terblend® N NM-21 EF Gray 38058 ABS+PA (Dry)
Description: Terblend® N NM-21 EF is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures. The enhanced flowability enables excellent processability and sur..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/A
Styrolution Terblend® S NM-31 ASA / PA
Terblend® S is a UV-stabilized ASA/PA blend with high impact strength, easy flow and pronounced color fastness. It is especially suitable for unpainted highly UV-exposed automotive interior parts..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature -20.0 °C
30.9 ft-lb/in²
<br>@Temperature -4.00 °F
80x10x4; ISO 180/1A
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded
Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar.
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
partial break; b.o. ISO 180-A
Covestro Makrolon® Rx1851 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
partial break; DAM; ISO 180/1A
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610 &nbsp;(Unverified Data**)
Zytel® RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is a black, unreinforced, toughened and heat stabilised r..
Izod Impact, Notched (ISO) 65.0 kJ/m²
<br>@Temperature 23.0 °C
30.9 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® ML6240 PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas..
Copyright © lookpolymers.com All Rights Reserved