| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® 104 PC (Europe-Africa-Middle East)
LEXAN 104 is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatibility informati..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in ..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXD101R PC (Europe-Africa-Middle East)
Transparent/translucent PC for light diffusion special effects. Thicker sections without sinks. Internal mold release. Pigment package may affect properties. Application testing always recommended..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXD103 PC
FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the ..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXD951A PC
Visual effetcs diffusion, flame retardant PC with low/medium flow good for extrusion/injection molding applications. Ideal for light management platforms that require hiding power and transmission.T..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXE144H PC
FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXE163R PC (Europe-Africa-Middle East)
LEXAN FXE163R is a transparent/translucent UV stabilized, medium viscosity grade for special effects with fluorescent appearance. Color package may affect performance. LEXAN FXE163R contains a relea..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® GLX143 PC (Europe-Africa-Middle East)
Lexan* GLX resin is a medium viscosity grade which is an excellent candidate for applications with high optical quality requirements, such as automotive glazing applications. Available in transparen..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Asia Pacific)
High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® ML7690 PC (Europe-Africa-Middle East)
LEXAN ML7690 is a high viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN ML7690 is available in transparent, translucent and opaque colours...
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® OQ2220 PC
Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent production control conditions.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
|
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT
(Unverified Data**)
Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXRL0662 PC
Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. ..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXRL0662 PC
Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. ..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXD144R PC (Europe-Africa-Middle East)
LEXAN FXD144R is a transparent/translucent medium viscosity grade for light diffusion effects. FDA compliant. Internal mold release. The color package may affect performance.This data was supplie..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXD163R PC (Europe-Africa-Middle East)
FXD163R is a Lexan PC Transparent grade in our VisualFX Portfolio. It is a light Diffusion effect, developed for today´s Aesthetic Differentiation Needs. Color package may effect properties, Ap..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
|
DSM Stapron® E EM 605 Polycarbonate/PET Blend (European Grade)
(discontinued **)
Information provided by DSM.
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC0700 PC (Asia Pacific)
PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC1000 PC (Europe-Africa-Middle East)
PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC1000R PC (Europe-Africa-Middle East)
PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC1003R PC
PC1003R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was ..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC1800 PC (Europe-Africa-Middle East)
PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold ..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC1800R PC (Asia Pacific)
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
ISO R 180 |
|
Styron Pulse® A35-105 PC/ABS
PULSEâ„¢ A35-105 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature.Information provided by DowThis product line was spun off f..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
33.3
ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
|
Covestro Makrolon® 1881 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Impact modified• Imp..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
33.3
ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
|
Covestro Makrolon® 2405 MAS056 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
33.3
ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
|
Covestro Makrolon® 2405 MAS057 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
partial break; DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**)
Zytel® RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is an unreinforced and toughened resin for injection molding..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature -40.0 °C |
33.3
ft-lb/in² @Temperature -40.0 °F |
50% RH; ISO 180 |
|
Solvay Specialty Polymers Amodel® EXT-1800 Polyphthalamide, extrusion
(discontinued **)
AMODEL EXT-1800 was developed specifically for the extrusion process. Unlike the grades targeted for injection molding, AMODEL EXT-1800 resin can be successfully extruded into tube, pipe, sheet, fil..
|
|||