Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 4.76 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycolac® GPM5500F ABS (Europe-Africa-Middle East)
CYCOLAC GPM5500F is a multi purpose injection moulding grade, providing a favourable balance of engineering properties and is FDA and European Directive 2002/72/EC (FCEU) compliant for food contac..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycolac® GPM5500U ABS (Europe-Africa-Middle East)
CYCOLAC GPM5500U is a UV stabilized multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500U has a wide processing window. It is recommended..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1...
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® FXG173R PC
This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle ..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -40.0 °C
4.76 ft-lb/in²
<br>@Temperature -40.0 °F
ISO 180/1A
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT &nbsp;(Unverified Data**)
Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180
LG Chemical XR-472 ABS, High Heat Resistance, High Gloss
Information Provided by LG Chem
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
cond.; ISO 180-1A
Lanxess Durethan® A 30 S H3.0 000000 Nylon 66, Injection Molding
PA 66, non-reinforced, injection moldingInformation provided by LANXESS.
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
<br>@Temperature 23.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature 73.4 °F
cond.; ISO 180-1A
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180-1A
Lanxess Durethan® BC 30 S 000000 Nylon 6
PA 6, non-reinforced, injection moldingInformation provided by LANXESS.
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180-1A
Lanxess Durethan® BKV 130 CS DUS008 600091 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fiber, injection molding, impact modifiedInformation provided by LANXESS.
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
d.a.m.; ISO 180-1A
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified
PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180-1A
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
<br>@Temperature -40.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -40.0 °F
d.a.m.; ISO 180-1A
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS.
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
d.a.m.; ISO 180-1U
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
cond.; ISO 180-1A
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced
PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
<br>@Temperature 23.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature 73.4 °F
d.a.m.; ISO 180-1A
Lanxess Durethan® ECO BV 30 H2 900500 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS.
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® 357 PBT
PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180/1A
Eurotec® Tecomid® NA40 GR30 NL PA 6.6 30% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecopet® PT70 GR30 NL100 PR PET, 30% glass fiber reinforced, high heat stabilized, natural, fast crystallization grade
Information provided by Eurotec®
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecotek® PC44 GR003 ZG70 PC, unfilled, flame retardant - halogen (RoHS compliant), light grey
Information provided by Eurotec®
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher ..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66 &nbsp;(Unverified Data**)
Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -40.0 °C
4.76 ft-lb/in²
<br>@Temperature -40.0 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612 &nbsp;(Unverified Data**)
Zytel® FE5382 BK276 is a 33% glass fiber reinforced, heat stabilized, black polyamide 612 resin developed for electrical bobbins and encapsulation applications.Information provided by DuPont Perfor..
Copyright © lookpolymers.com All Rights Reserved