| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East)
CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Thickness 4.00 mm,<br> Temperature -20.0 °C
|
5.71
ft-lb/in² <br>@Thickness 0.157 in,<br> Temperature -4.00 °F
|
ISO 180 |
|
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound
PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 0.000 °C
|
5.71
ft-lb/in² <br>@Temperature 32.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Geloy HRA222 ASA (Europe-Africa-Middle East)
GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material.This data was supplied by..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXE144H PC
FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXM4701 PPC (Asia Pacific)
LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Asia Paci..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® IFX2420Z PC (Asia Pacific)
Lexan* IFX2420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware applications specifically for welding. This grades ..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® IR2520 PC
General purpose polycarbonate with melt flow rate of 8.5.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
DuPont Performance Polymers Delrin® 500T BK602 Acetal Homopolymer
(Unverified Data**)
Delrin® 500T BK602 is a toughened, medium viscosity acetal homopolymer resin with impact resistance similar to Delrin® 100. It can be used in parts requiring noise reduction.Information provided b..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXD9945A PC (Europe-Africa-Middle East)
UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
50%RH; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**)
Zytel® 70G30HSL BK039B is a 30% glass reinforced, heat stabilized, black nylon 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl PX9406N PPE+HIPS (Europe-Africa-Middle East)
Noryl PX9406N is an unfilled, halogen free (according VDE/DIN 472 part 813) flame retardant material with medium heat resistance. This material is V0 at 1.0 mm according to UL94.This data was suppli..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC0700 PC
PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC1800 PC
PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold ..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC2200 PC (Asia Pacific)
PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC2203R PC
PC2203R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/A |
|
Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Dry)
Description: Terblend® N NG-02 EF is a glass fiber reinforced UV stabilized ABS/PA blend with excellent dimensional stability and high impact strength. The enhanced flowability enables excellent ..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP
Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180 |
|
Polyram RamSter PF306G6 PBT, 30% Glass Fiber
30% Glass fiber reinforced, low viscosity PBT for injection molding applications.Information provided by Polyram.
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180 |
|
Total PPC 9612 Polypropylene, Heterophasic Copolymer, Injection Molding
This product is a Total Ecosolutions grade.Polypropylene PPC 9612 has been developed specifically for the injection molding of crates and is characterized by a high Melt Flow index of 20 g/10 min. ..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Thickness 0.126 in,<br> Temperature -22.0 °F
|
complete break; b.o. ISO 180-A |
|
Covestro Makrolon® 2407 MAS070 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Thickness 0.126 in,<br> Temperature -22.0 °F
|
complete break; b.o. ISO 180-A |
|
Covestro Makrolon® 2407 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Thickness 0.126 in,<br> Temperature -22.0 °F
|
complete break; b.o. ISO 180-A |
|
Covestro Makrolon® 3107 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecodur® PB70 GR20 NL IH PBT 20% glass fiber reinforced, impact modified
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NA40 GR40 NL PA 6.6 40% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NA43 GR25 NL TD43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, high impact, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -40.0 °C
|
5.71
ft-lb/in² <br>@Temperature -40.0 °F
|
ISO 180 |
|
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM
Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180 |
|
Ascend Performance Materials Vydyne® R533T Nylon 66, Translucent, 33% Glass Filled, Conditioned (2.5% Moisture)
The Vydyne® R533T is a translucent 33% glass reinforced heat stabilized Nylon 66 product specifically designed for use in power steering reservoirs and other applications where chemical resistance,..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -40.0 °C
|
5.71
ft-lb/in² <br>@Temperature -40.0 °F
|
ISO 180 |
|
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180 |
|
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Geloy FXW710SK ASA/SAN (Europe-Africa-Middle East)
GELOY FXW710SK is an ASA/SAN injection moulding grade. It is suitable for those applications that require sparkle colour effects.This data was supplied by SABIC-IP for the Europe-Africa-Middle East ..
|
|||