| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East)
This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® C4215HF PC+ABS (Europe-Africa-Middle East)
Cycoloy C4215HF is a 15% glass reinforced, non-FR PC+ABS grade with high heat resistance, excellent strength and rigidity with good cosmetic apprearance. It combines good processability with a low s..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® ML6031 PC Copolymer (Asia Pacific)
High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacific ..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature 23.0 °C |
3.33
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® CRT3370 ABS (Europe-Africa-Middle East)
CYCOLAC CRT3370 is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow char..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -40.0 °C |
3.33
ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**)
Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
ISO 180-1A |
|
Ineos ABS Lustran® ABS 450 Injection Molding Grade
Lustran® ABS 450 has medium impact strength, high flow, and is injection molding grade.
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl PX9406N PPE+HIPS (Europe-Africa-Middle East)
Noryl PX9406N is an unfilled, halogen free (according VDE/DIN 472 part 813) flame retardant material with medium heat resistance. This material is V0 at 1.0 mm according to UL94.This data was suppli..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature 23.0 °C |
3.33
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Xylex X8419 PC+POLYESTER
Low-medium flow, suitable for blow molding, injection molding, extrusion.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP
Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific)
Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
|
Styrolution Terluran® GP-25 ABS
Terluran GP-25 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings se..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature 23.0 °C |
3.33
ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
|
Sax Polymers SAXLAC 108 GF17 Acrylonitrile Butadiene Styrene, 17% Glass Fiber
Saxalac 108 GF17 is a 17% glass fiber reinforced ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data te..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -40.0 °C |
3.33
ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
|
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded
AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -40.0 °C |
3.33
ft-lb/in² @Temperature -40.0 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
|
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded
BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1A |
|
Eurostar Staramide PF003IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide PF003IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF1003HI005)Information provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature 23.0 °C |
3.33
ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
|
Eurostar Starflam AFR450B PA66, 25% Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR450B is a Flame Retardant, 25% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
|
Eurotec® Tecodur® PB70 BK001 HS PBT, unfilled, improved impact, heat stabilized, black
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature 23.0 °C |
3.33
ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
|
Eurotec® Tecomid® NB40 GR20 NL XA60 PA6, 20% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature 23.0 °C |
3.33
ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
|
Eurotec® Tecodur® PB70 GR20 NL CA 01 PBT/PET 20% glass fiber reinforced
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature 23.0 °C |
3.33
ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
|
Eurotec® Tecoform® PO30 GR20 NL HS POM, 20% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
|
Eurotec® Tecomid® NA40 MR15 NL IL PA 6.6 15% mineral reinforced, impact modified
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature 23.0 °C |
3.33
ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
|
Eurotec® Tecomid® NB40 GR15 NL PA 6 15% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature 23.0 °C |
3.33
ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
|
BASF Ultraform® N2320 U035 POM
Description: Is a POM, UV-stabilized injection-molding grade.Information provided by BASF
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
|
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, Conditioned
Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature 23.0 °C |
3.33
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Europe-Africa-Middle East)
PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the E..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -30.0 °C |
3.33
ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
|
DuPont Performance Polymers Crastin® LW9030 BK851 PBT
(Unverified Data**)
Crastin® LW9030 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp..
|
|||
| Izod Impact, Notched (ISO) |
7.00
kJ/m² @Temperature -40.0 °C |
3.33
ft-lb/in² @Temperature -40.0 °F |
ISO 180/1A |
|
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**)
Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers
|
|||