Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 7.14 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycolac® S701 ABS (Europe-Africa-Middle East)
CYCOLAC S701 is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appli..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® C1000 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1000 is a PC+ABS blend developed with emphasis on excellent processing efficiency while maintaining good heat resistance and impact ductility. It is an excellent material choice for a wide ..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Thickness 4.00 mm,
Temperature -20.0 °C
7.14 ft-lb/in²

@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound
PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Europe-Africa-Middle East)
CYCOLOY LG9000 is a low gloss PC+ABS injection moulding grade. LG9000 combines good impact / heat and UV resistance with a low gloss surface appearence. It is suitable for automotive interior applic..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Geloy XTWM206 ASA (Asia Pacific)
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Asia Pacific regio..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® ML6413 PC (Europe-Africa-Middle East)
Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Nilit Nilamid A3 H ZB High Impact PA66
Description: Nilamid A3 H ZB is high impact NYLON 66. The product maintains excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas ..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
ISO 80
LG Chemical LG-703A ABS, Low Gloss, General Purpose
Information Provided by LG Chem
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
ISO 80
LG Chemical LI-921 ASA, Extrusion, High Stiffness
Information Provided by LG Chem
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
ISO 80
LG Chemical LI-941 ASA, Extrusion, High Heat Resistance
Information Provided by LG Chem
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
ISO 180-1A
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers
PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
d.a.m.; ISO 180-1A
Lanxess Durethan® BKV 50 H2.0 EF DUS30 901510 Nylon 6, Glass Fiber Reinforced
PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -20.0 °C
7.14 ft-lb/in²

@Temperature -4.00 °F
ISO 180-1A
Ineos ABS Lustran® ABS 595CP Refrigeration and Extrusion Grade
Lustran® ABS 595CP is refrigeration and extrusion grade, resistant to cyclopentane, and has high impact strength.
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
cond.; ISO 180-1A
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced
PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
ISO 180-1A
Lanxess Durethan® BKV 325 Z H2.0 901510 Nylon 6, 25% Glass Fibers
PA 6, 25% glass fibers, blow molding, impact modified, heat-ageing stabilized
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
ISO 180
LyondellBasell Hostacomâ„¢ CA270G Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CA270G fractional melt flow, 140 MPa flexural modulus, UV-stabilized thermoplastic elastomeric olefin (TEO) resin has an excellent combination of grain retention characte..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Ultem ATX100R PEI (Europe-Africa-Middle East)
Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB Listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Ultem HATX100 PEI+PCE (Europe-Africa-Middle East)
Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styrolution Novodur® M205FC ABS
Novodur HD M205FC is an injection molding grade especially suitable for medical applications providing enhanced stiffness.Information provided by Styrolution
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -40.0 °C
7.14 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® XD1507S PBT+PC (Europe-Africa-Middle East)
XENOY XD1507S is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties, designed for self coloured, optiwall bumper facias.This data was supplie..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Verton RV008ESV_GY7E072 PA 66
Preliminary data for 40% long glass fiber filled, single color pellet gray, PA66This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
ISO 180-A
Covestro Bayblend® FR3001 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1A
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded
AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Eurotec® Tecotek® PC43 GR003 TD70 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, light grey
Information provided by Eurotec®
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
ISO 180
BASF Ultramid® 82335G HS BK 102 50% Glass Filled PA6 (Dry)
Description: Ultramid 8235G HS BK-102 is a heat stabilized, pigmented black, 50% glass fiber reinforced PA6 injection molding compound offering excellent level of strength, stiffness, high temperatu..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -40.0 °C
7.14 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610  (Unverified Data**)
Zytel® RS 30G30HSL BK038A is a lubricated, heat stabilized, 30% glass fiber reinforced black polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on po..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Europe-Africa-Middle East)
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Thermotuf PF003IX1 PA 6 (Europe-Africa-Middle East)
High Impact Nylon 6 compound containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Copyright © lookpolymers.com All Rights Reserved