| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EX1036T PC (Europe-Africa-Middle East)
LEXAN EX1036T is a transparent, high viscosity, UV stabilized polycarbonate grade and contains a release agent to ensure easy processing. LEXAN EX1036T is produced under tight color specifications.T..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in ..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXD141 PC (Europe-Africa-Middle East)
LEXAN FXD141 is a transparent/translucent medium viscosity grade for light diffusion effects. The color package may affect performance.This data was supplied by SABIC-IP for the Europe-Africa-Middl..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXD951A PC
Visual effetcs diffusion, flame retardant PC with low/medium flow good for extrusion/injection molding applications. Ideal for light management platforms that require hiding power and transmission.T..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXD9945A PC
UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXE101 PC (Europe-Africa-Middle East)
Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXE161R PC (Europe-Africa-Middle East)
LEXAN FXE161R is a transparent/translucent medium viscosity grade for special effects with fluorescent appearance. Color package may affect performance. LEXAN FXE161R contains a release agent to ens..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXE1643 PC (Europe-Africa-Middle East)
LEXAN FXE1643 is an extrusion blow moulding grade in visual effect Energy especially developed for refillable containers for water, juices and milk. It offers high melt strength, impact resistance a..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Asia Pacific)
High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Europe-Africa-Middle East)
High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® IFX2420Z PC (Asia Pacific)
Lexan* IFX2420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware applications specifically for welding. This grades ..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® IM1063 PC (Europe-Africa-Middle East)
Lexan* IM1063 is a impact modified polycarbonate gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® OQ2220 PC
Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent production control conditions.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer (Europe-Africa-Middle East)
Transparent weatherable PC copolymer for blowmolding/extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
|
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT
(Unverified Data**)
Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXRL0662 PC
Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. ..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXRL0683 PC Copolymer
11 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXE143R PC (Europe-Africa-Middle East)
LEXAN FXE143R is a medium viscosity multi purpose UV stabilized grade for visual effects in "energy". The material contains a release agent to ensure easy processing.This data was supplied by SABIC-..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
|
DSM Stapron® E EM 605 Polycarbonate/PET Blend (European Grade)
(discontinued **)
Information provided by DSM.
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC0800 PC
PC0800 resin is a low flow (MFR = 8 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC1000 PC (Asia Pacific)
PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC1000 PC (Europe-Africa-Middle East)
PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC1000R PC (Europe-Africa-Middle East)
PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC1800 PC (Europe-Africa-Middle East)
PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold ..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC1800R PC (Asia Pacific)
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East)
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
33.3
ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
|
Covestro Makrolon® 1881 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Impact modified• Imp..
|
|||
| Izod Impact, Notched (ISO) |
70.0
kJ/m² @Temperature 23.0 °C |
33.3
ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXE144H PC (Europe-Africa-Middle East)
FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe..
|
|||