| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Thickness 4.00 mm,<br> Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Thickness 0.157 in,<br> Temperature -22.0 °F
|
ISO 180/1A |
|
Polimeri Europa Edistir ICE R 830D Polystyrene
Environmental stress cracking resistant (ESCR) HIPS. ICE PD R 830D combines high impact strength with an improved chemical resistance to oils, fats and chemical agents, such as detergents for both i..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Thickness 4.00 mm,<br> Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Thickness 0.157 in,<br> Temperature 73.4 °F
|
ISO 180/1A |
|
Polimeri Europa Edistir R 540E Polystyrene
HIPS with high stiffness, matt surface finish and good heat resistance. Suitable for general extrusion of thick sheets and profiles. Also used for injection
moldings. Designation: Thermoplastics IS..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East)
CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Thickness 4.00 mm,<br> Temperature -20.0 °C
|
3.81
ft-lb/in² <br>@Thickness 0.157 in,<br> Temperature -4.00 °F
|
ISO 180 |
|
Premix Thermoplastics PRE-ELEC® ABS 1415 Conductive Thermoplastic Compound
PRE-ELEC® ABS 1415 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® ABS..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Europe-Africa-Middle East)
PC+ABS, of non-chlorinated & non brominated flame retardant with metallic or pearlescent appearance. MAGIX color package may affect performance.This data was supplied by SABIC-IP for the Europe-Afri..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® FXC630FE PC+ABS (Europe-Africa-Middle East)
Multi purpose flame retarded PC+ABS injection moulding grade, suitable for those applications that require ferrite colour effects.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
50%RH; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**)
Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180-1A |
|
Ineos ABS Lustran® ABS E112LG Pellets
Lustran® ABS E112LG is extrusion grade for low gloss surfaces. It is used for the production of molded plastic articles.
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -40.0 °C
|
3.81
ft-lb/in² <br>@Temperature -40.0 °F
|
ISO 180 |
|
LyondellBasell Hifaxâ„¢ CA287AHF Thermoplastic Polyolefin Elastomer
Description: Hifax â„¢ CA287AHF is a thermoplastic polyolefin elastomer suitable for automotive exterior partsFeatures: Good StiffnessGood ProcessabilityGood Impact ResistanceGood Colorability Pa..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl PX7446 PPE+PS
This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® V9500GW PET+PC (Europe-Africa-Middle East)
Unfilled Flameretardant PET/PC blend for GWIT.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -40.0 °C
|
3.81
ft-lb/in² <br>@Temperature -40.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Thermocomp RF006XXP PA 66 (Europe-Africa-Middle East)
30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -20.0 °C
|
3.81
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 180/1A |
|
Borealis GB311U Polypropylene Compound, Glass Fiber Reinforced
GB311U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. ..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -20.0 °C
|
3.81
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 180 |
|
Total PPC 1640 Polypropylene, Heterophasic Copolymer, Non-pressure Pipes
Polypropylene PPC 1640 is a nucleated heterophasic (block) copolymer with a Melt Flow index of 0.3 g/10 min. This resin has a long-term heat stabilization package. It exhibits high stiffness in co..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -40.0 °C
|
3.81
ft-lb/in² <br>@Temperature -40.0 °F
|
ISO 180/1A |
|
DSM Stanyl® TW275F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
80x10x4; ISO 180/1A |
|
Eurostar Staramide ACF4 PA66, 20% Carbon Fiber Reinforced, Heat stabilized, Injection Molding
Staramide ACF3 is a 20% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
80x10x4; ISO 180/1A |
|
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded
AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -40.0 °C
|
3.81
ft-lb/in² <br>@Temperature -40.0 °F
|
80x10x4; ISO 180/1A |
|
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded
AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
80x10x4; ISO 179/1eA |
|
Eurostar Starflam RF0069 PA66, 30% Glass Fiber, Flame Retardant, Injection Molded
Starflam RF0069 is a Flame Retardant, 30% Glass Reinforced Polyamide 66 Injection Molding Resin (also known as PA66 30V U2 Z79 or RF1006Z590)Information provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecodur® PB70 GR30 NL CA 01 PBT/PET 30% glass fiber reinforced
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecodur® PB70 GR30 NL XA70 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NA40 GR25 GR003 XA70 PA6.6, 25% glass fiber reinforced, flame retardant - halogen free (RoHS compliant), heat stabilized, grey RAL 7035
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NA43 GR25 NL XA43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, heat stabilized, natural, UL registered
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NT40 CR30 BK111 HS PPA, 30% carbon fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
80x10x4; ISO 180/1A |
|
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded
BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecodur® PB70 GR45 NL100 HS01 PBT/PET, 45% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NA40 GR25 NL PA 6.6 25% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NA40 GR20 NL PA 6.6 20% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® VX4015 PBT (Europe-Africa-Middle East)
VALOX VX4015 is a 15% glass reinforced PBT injection moulding resin, with excellent hydrolytical stability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||