| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Thickness 4.00 mm,<br> Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Thickness 0.157 in,<br> Temperature 73.4 °F
|
ISO 180/1A |
|
Polimeri Europa Sinkral® B 432/E ABS Resin
Sinkral B 432/E is a general purpose extrusion grade which exhibits a good balance between rigidity and toughness. Designation: Thermoplastic ISO 2580-ABS 1,EGN,105-04-16-20Applications: Large sheet..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Geloy HRA222 ASA (Europe-Africa-Middle East)
GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material.This data was supplied by..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature -30.0 °C
|
8.09
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East)
XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**)
Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**)
Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature -20.0 °C
|
8.09
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 180-1A |
|
Ineos ABS Lustran® ABS 970
Lustran® ABS 970 has high impact strength and good paintability.
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature -30.0 °C
|
8.09
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Xylex X7503HP PC+POLYESTER (Europe-Africa-Middle East)
Clear PC-Siloxane copolymer + Polyester alloy, USA Food ContactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/A |
|
Styrolution Novodur® H702 ABS
Novodur H702 is a high heat, high gloss injection molding grade with very good flowabilityInformation provided by Styrolution
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/A |
|
Styrolution Novodur® H950 ABS
Novodur H950 is a very high heat injection molding grade with high gloss surface appearanceInformation provided by Styrolution
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
Styron DGF080.00 ESU Polypropylene
Overview: 10% glass filled polypropyleneNaturalMedium flowHeat ResistantInformation provided by Styron
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature -30.0 °C
|
8.09
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180 |
|
Styron MAGNUMâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Impact, High Heat, Blow Molding ABSInformation provided by Styron
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/A |
|
Styron Magnumâ„¢ 3525 Acrylonitrile Butadiene Styrene (ABS)
MAGNUMâ„¢ 3525 is a resin with excellent processing characteristics. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent processability with a stable..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature -30.0 °C
|
8.09
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/A |
|
Styron Magnumâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS)
MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines ex..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature -30.0 °C
|
8.09
ft-lb/in² <br>@Temperature -22.0 °F
|
Injection Molded; ISO 180/A |
|
Styron MAGNUMâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. It can be processed by injection molding, extrusion or thermoforming. The mass (c..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
Sax Polymers SAXAMID 136F3Q32 Nylon 6, 15% Glass Fiber
SAXAMID 136F3Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 15% glass fibers with very high impact properties. Beside the high impact strength at low temperatures ..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
Sax Polymers SAXAMID 136F4Q32 Nylon 6, 20% Glass Fiber
SAXAMID 136F4Q32 is a high impact-modified polyamide 6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature -40.0 °C
|
8.09
ft-lb/in² <br>@Temperature -40.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Verton NV0041EV_GY7E147 PC+ABS
Preliminary data for 20% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature -30.0 °C
|
8.09
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific)
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl GTX GTX976 PPE+PA (Europe-Africa-Middle East)
NORYL GTX976 is a material especially designed for electrostatic painting and powder coating applications. This material combines high impact performance with conductivity in an unique way.This data..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/A |
|
Styron Magnumâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS)
MAGNUMâ„¢ 3325 MT is resin with excellent processing characteristics and a matt surface finish. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent p..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature -30.0 °C
|
8.09
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl MX5569 PPE+PS
PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature -40.0 °C
|
8.09
ft-lb/in² <br>@Temperature -40.0 °F
|
50%RH; ISO 180/1A |
|
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**)
Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature -30.0 °C
|
8.09
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NA40 GR30 NL IH PA6.6, 30% glass fiber reinforced, impact modified, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature -30.0 °C
|
8.09
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NB40 GR50 NL PA 6 50% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180 |
|
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature -30.0 °C
|
8.09
ft-lb/in² <br>@Temperature -22.0 °F
|
DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**)
Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide..
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**)
Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Izod Impact, Notched (ISO) |
17.0
kJ/m² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||