Mechanical Properties Metric English Comments
Tensile Strength at Break 9.40 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
1360 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
200 mm/min Across Flow; DIN 53504
PolyOne OnFlex™ HT 50A-3S2099 Thermoplastic Elastomer (TPE)
OnFlex™ HT thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds is specially formulated to deliver very good compression set performance at..
Tensile Strength at Break 9.40 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
1360 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
200 mm/min Across Flow; DIN 53504
PolyOne OnFlex™ HT 70A-3S2103 Thermoplastic Elastomer (TPE)
OnFlex™ HT thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds is specially formulated to deliver very good compression set performance at..