Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 16000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa

@Temperature 175 °C
16000 psi

@Temperature 347 °F
ISO 527
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont..
Tensile Strength at Break 110 MPa

@Temperature 175 °C
16000 psi

@Temperature 347 °F
ISO 527
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com..
Tensile Strength at Break 110 MPa

@Temperature 23.0 °C
16000 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66  (Unverified Data**)
Zytel® FE270038 is a 40% glass fiber/mineral reinforced, heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.Information provided by DuPont Performan..
Tensile Strength at Break 110 MPa

@Temperature 23.0 °C
16000 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL BK261 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 for injection molding. It has excellent surface appearance and gloss.Information provided by Du..
Tensile Strength at Break 110 MPa

@Temperature 23.0 °C
16000 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6  (Unverified Data**)
Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 110 MPa

@Temperature 23.0 °C
16000 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6  (Unverified Data**)
Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 110 MPa

@Temperature 60.0 °C
16000 psi

@Temperature 140 °F
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant
Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low..
Tensile Strength at Break 110 MPa

@Temperature 150 °C
16000 psi

@Temperature 302 °F
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 110 MPa

@Temperature 60.0 °C
16000 psi

@Temperature 140 °F
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced
Polyamide 12 (PA12) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Tensile Strength at Break 110 MPa

@Temperature 90.0 °C
16000 psi

@Temperature 194 °F
LATI Latamid 66 E21 K/30 PA 66, 30% Carbon Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Carbon fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastic..
Tensile Strength at Break 110 MPa

@Temperature 60.0 °C
16000 psi

@Temperature 140 °F
LATI Latamid 66 H2 G/35-V0KB3 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Strength at Break 110 MPa

@Temperature 120 °C
16000 psi

@Temperature 248 °F
LATI Latamid 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Strength at Break 110 MPa

@Temperature 60.0 °C
16000 psi

@Temperature 140 °F
LATI Lapex A G/20 PES, 20% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Tensile Strength at Break 110 MPa

@Temperature 23.0 °C
16000 psi

@Temperature 73.4 °F
LATI Lapex R G/20 PPSU, 20% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Strength at Break 110 MPa

@Temperature 23.0 °C
16000 psi

@Temperature 73.4 °F
LATI Laramid G/15 PPA, 15% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Strength at Break 110 MPa

@Temperature 90.0 °C
16000 psi

@Temperature 194 °F
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 110 MPa

@Temperature 150 °C
16000 psi

@Temperature 302 °F
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 110 MPa

@Temperature 150 °C
16000 psi

@Temperature 302 °F
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..
Tensile Strength at Break 110 MPa

@Temperature 120 °C
16000 psi

@Temperature 248 °F
LATI Larton G/40 I6 PPS, 40% Glass Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers. Good elongation. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Strength at Break 110 MPa

@Temperature 60.0 °C
16000 psi

@Temperature 140 °F
LATI Lasulf G/30 PSU, 30% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Tensile Strength at Break 110 MPa

@Temperature 120 °C
16000 psi

@Temperature 248 °F
LATI Latamid SP1 G/50 PA 6.10, 50% Glass Fiber Reinforced
Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
Tensile Strength at Break 110 MPa

@Temperature 60.0 °C
16000 psi

@Temperature 140 °F
LATI Later 4 K/30 PBT, 30% Carbon Fiber Reinforced
Polybutylene Terephthalate (PBT) based compound. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplasti..
Tensile Strength at Break 110 MPa

@Temperature 90.0 °C
16000 psi

@Temperature 194 °F
LATI Latigloss 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Strength at Break 110 MPa

@Temperature 60.0 °C
16000 psi

@Temperature 140 °F
LATI Latilon 28D K/20 PC, 20% Carbon Fiber Reinforced
Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b..
Tensile Strength at Break 110 MPa

@Temperature 23.0 °C
16000 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Minlon® FE6190 BK086 Nylon 66
Minlon® FE6190 BK086 is a 36% mineral/glass reinforced, heat stabilized, black polyamide resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 110 MPa

@Temperature 23.0 °C
16000 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 110 MPa

@Temperature -40.0 °C
16000 psi

@Temperature -40.0 °F
ISO 527
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT  (Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..
Tensile Strength at Break 110 MPa

@Temperature 23.0 °C
16000 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® BM70G15HSLR BK537 Nylon 66
Zytel® BM70G15HSLR BK537 is a 15% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 110 MPa

@Temperature 23.0 °C
16000 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/25-V0KB4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Strength at Break 110 MPa

@Temperature 23.0 °C
16000 psi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Rynite® 940 BK505 PET  (Unverified Data**)
Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers