Polymer Property : Tensile Strength, Yield = 138 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 138 MPa

@Thickness 1.57 mm
20000 psi

@Thickness 0.0620 in
LW; ASTM D638
Industrial Laminates/Norplex NP842 Paper Base Laminate  (discontinued **)
Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP842 is semi-conductive on the surfaces and through the laminate.Thickness Tested: 0..
Tensile Strength, Yield 138 MPa

@Thickness 1.57 mm
20000 psi

@Thickness 0.0620 in
LW; ASTM D638
Industrial Laminates/Norplex NP610 Paper Base Laminate
Description: Phenolic paper based grade for mechanical applications. Good tensile, compressive and flexural strength. Primarily a machining material, but may be hot punched up to .093" thick.Thickne..
Tensile Strength, Yield 138 MPa

@Thickness 1.57 mm
20000 psi

@Thickness 0.0620 in
LW; ASTM D638
Industrial Laminates/Norplex NP660 Paper Base Laminate
Description: Lower cost paper phenolic NEMA Grade XP. Uses natural kraft paper without pigmented cover sheet. Warm to hot punching. UL listed. Thickness Tested: 0.062", 0.125" & 0.500"
Tensile Strength, Yield 138 MPa

@Diameter 25.4 mm
20000 psi

@Diameter 1.00 in
Rod H02
Mueller Ecostreamâ„¢ C36300 Copper Zinc Lead Alloy
As one of the low lead alloys offered in the EcoStream™ family of products, Mueller Brass Company’s C36300 alloy provides a viable alternative to those manufacturers who are manufacturing ..
Tensile Strength, Yield 138 MPa

@Temperature 177 °C
20000 psi

@Temperature 351 °F
[+/-45°]; Resin Content=27%, Fiber Volume=66%
Hexcel® HexPly® F650 Bismaleimide Resin with IM6 Fiber
Composition: IM6 Fiber, 12K, G sizes, UD Tape - 145 g/m2Information provided by HexCel
Tensile Strength, Yield >= 138 MPa

@Strain 0.200 %,
Thickness <=63.5 mm
>= 20000 psi

@Strain 0.200 %,
Thickness <=2.50 in
Carlson 70 30 Cu Ni Copper-Nickel Alloy
General DescriptionCarlson alloy 70 30 Cu Ni is a copper nickel alloy with excellent resistance to corrosion and erosion. It is strong and ductile. 70 30 Cu Ni is utilized in areas where high temp..
Tensile Strength, Yield 138 MPa

@Temperature -40.0 °C
20000 psi

@Temperature -40.0 °F
ASTM D638
BASF Ultramid® 8270 HS BK 102 PA6 (Dry)
Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex..
Tensile Strength, Yield 138 MPa

@Temperature 760 °C
20000 psi

@Temperature 1400 °F
ASTM E8
ATI Allegheny Ludlum 309 Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Tensile Strength, Yield 138 MPa

@Temperature 1090 °C
20000 psi

@Temperature 2000 °F
Vacuum
ATI Wah Chang Nb/Nb Alloy C-103
This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig..
Tensile Strength, Yield >= 138 MPa

@Strain 0.200 %
>= 20000 psi

@Strain 0.200 %
PSM Industries PolyAlloys MIM-316L sintered Stainless Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..