| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield |
172
MPa @Strain 0.200 %, Temperature 100 °C |
24900
psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
|
Outokumpu 4438 High Performance Austenitic Stainless Steel
Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,..
|
|||
| Tensile Strength, Yield |
172
MPa @Strain 1.00 %, Temperature 300 °C |
24900
psi @Strain 1.00 %, Temperature 572 °F |
EN min.; EN 10002-5 |
|
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For ..
|
|||
| Tensile Strength, Yield |
>=
172
MPa @Strain 0.200 % |
>=
25000
psi @Strain 0.200 % |
|
|
PSM Industries PolyAlloys MIM-4605 sintered Low Alloy Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..
|
|||
| Tensile Strength, Yield |
172
MPa @Diameter 12.7 - 25.4 mm |
25000
psi @Diameter 0.500 - 1.00 in |
Rod H02 |
|
Mueller Ecostreamâ„¢ C36300 Copper Zinc Lead Alloy
As one of the low lead alloys offered in the EcoStream™ family of products, Mueller Brass Company’s C36300 alloy provides a viable alternative to those manufacturers who are manufacturing ..
|
|||
| Tensile Strength, Yield |
>=
172
MPa @Treatment Temp. 1010 - 1090 °C, Strain 0.200 % |
>=
25000
psi @Treatment Temp. 1850 - 2000 °F, Strain 0.200 % |
Heat Treatment |
|
Schmolz + Bickenbach UGIMA 303 UX® Stainless Steel Bar
Description: 303 UGIMA UX® is an improved machining grade produced only by Ugitech, providing the ultimate level of machinability available in an austenitic stainless steel. 303 UGIMA UX® feat..
|
|||
| Tensile Strength, Yield |
172
MPa @Temperature 760 °C |
25000
psi @Temperature 1400 °F |
Vacuum |
|
ATI Wah Chang Nb/Nb Alloy C-103
This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig..
|
|||
| Tensile Strength, Yield |
>=
172
MPa @Strain 0.200 % |
>=
25000
psi @Strain 0.200 % |
|
|
Carlson C 800H Nickel-Iron-Chromium Alloy
General DescriptionCarlson Alloy C 800 is a nickel-iron-chromium alloy, combining high strength with excellent resistance to oxidation and carburization at elevated temperatures. This alloy resists..
|
|||
| Tensile Strength, Yield |
172
MPa @Strain 0.200 % |
25000
psi @Strain 0.200 % |
|
|
PSM Industries PolyAlloys MIM-316L sintered Stainless Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..
|
|||