| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data)
Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data)
Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 1 m/s unlubricated |
|
Quadrant EPP Ertalon® 6 PLA PA 6, cast (ISO Data)
Unmodified cast nylon 6 grade exhibiting characteristics which come very close to those of Ertalon 66 SA. It combines high strength, stiffness and hardness with good creep and wear resistance, heat ..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 1 m/s unlubricated |
|
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data)
Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 1 m/s unlubricated |
|
Quadrant EPP Nylatron® GS PA 6 + MoS2, extruded (ISO Data)
The addition of MoS2 renders this material somewhat stiffer, harder and dimensionally more stable than Ertalon 66 SA, but results in some loss of impact strength. The nucleating effect of the molybd..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 1 m/s unlubricated |
|
Quadrant EPP Nylatron® GSM PA 6 + MoS2, cast (ISO Data)
Nylatron GSM contains finely divided particles of molybdenum disulphide to enhance its bearing and wear behaviour without impairing the impact and fatigue resistance inherent to unmodified cast nylo..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 1 m/s unlubricated |
|
Quadrant EPP Nylatron® LFG PA 6 + oil, cast (ISO Data)
Nylatron LFG (Lubricated Food Grade) is self-lubricating in the real meaning of the word, and has a FDA food contact compliant composition. The Nylatron LFG has been specially developed for non-lubr..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 1 m/s unlubricated |
|
Quadrant EPP Nylatron® MC901 PA 6, blue, cast (ISO Data)
This modified cast nylon 6 grade with its distinctive blue colour exhibits higher toughness, flexibility and fatigue resistance than Ertalon 6 PLA. It has proved to be an excellent material for gear..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data)
This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® 1000 antistatic PE-UHMW + carbon black (ISO Data)
By incorporating an effective carbon black grade, TIVAR 1000 antistatic offers the electrostatic dissipative properties often required for PE-UHMW components operating at high line speeds and convey..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® 1000 ASTL PE-UHMW + specific additives (ISO Data)
TIVAR 1000 ASTL, based on a PE-UHMW grade with extremely high molecular weight, has been specifically developed for tough anti-abrasion applications. TIVAR 1000 ASTL shows a higher wear and abrasion..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® 1000 EC PE-UHMW + specific additives (ISO Data)
TIVAR 1000 EC is a PE-UHMW grade containing specific additives rendering this material a lower surface resistivity than TIVAR 1000 antistatic, improving electrical conductivity and UV-resistance
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data)
TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C.
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data)
TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethyl..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data)
TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® Cleanstat PE-UHMW + specific additives (ISO Data)
TIVAR CleanStat is a PE-UHMW grade for use in food processing and pharmaceutical industries. It exhibits static dissipative properties and has a food contact compliant composition. Very good wear an..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® Dryslide PE-UHMW + internal lubricant + other additives (ISO Data)
Thanks to the lubricant built into a PE-UHMW matrix with higher molecular weight, TIVAR DrySlide offers a lower coefficient of friction and enhanced wear and abrasion resistance than TIVAR 1000. The..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® DS PE-UHMW + additives (ISO Data)
TIVAR DS is a modified PE-UHMW with extremely high molecular weight. The latter in combination with a particular manufacturing process result in a PE-UHMW grade with superior wear and abrasion resis..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® ECO PE-UHMW reprocessed (ISO Data)
This grade, partially composed of reprocessed PE-UHMW material, has an overall lower property level than the virgin TIVAR 1000 and a lower cost. Compared with virgin PE 500, however, it has a much b..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® H.O.T. PE-UHMW + specific additives (ISO Data)
TIVAR H.O.T. [Higher Operating Temperature] is formulated to maintain inherent PE-UHMW key properties over an extended service temperature range, in this way considerably increasing part life in low..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data)
This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data)
TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® SuperPlus PE-UHMW + specific additives (ISO Data)
TIVAR SuperPlus is a wear optimised, partially cross-linked PE-UHMW material with extremely high degree of polymerisation for use in most demanding applications and environments. When used for drain..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | at 0.1 m/s unlubricated |
|
Quadrant EPP TIVAR® TECH PE-UHMW + MoS2 (ISO Data)
This PE-UHMW grade with extremely high degree of polymerisation contains molybdenum disulphide, resulting in a material with improved wear resistance and sliding properties over TIVAR 1000.
|
|||
| Limiting Pressure Velocity | 0.0800 - 0.701 MPa-m/sec | 2280 - 20000 psi-ft/min | Average value: 0.398 MPa-m/sec Grade Count:7 |
|
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v..
|
|||
| Limiting Pressure Velocity | 0.0800 - 0.130 MPa-m/sec | 2280 - 3710 psi-ft/min | Average value: 0.101 MPa-m/sec Grade Count:3 |
|
Overview of materials for Nylon 66, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate..
|
|||
| Limiting Pressure Velocity | 0.0800 MPa-m/sec | 2280 psi-ft/min | without lubrication; MPC Test |
|
Manifattura Cattaneo PET Polyethylene Terephthalate
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
|
|||
| Limiting Pressure Velocity | 0.0800 - 1.33 MPa-m/sec | 2280 - 38000 psi-ft/min | Average value: 0.412 MPa-m/sec Grade Count:12 |
|
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
|
|||
| Limiting Pressure Velocity | 0.0800 - 0.193 MPa-m/sec | 2280 - 5500 psi-ft/min | Average value: 0.127 MPa-m/sec Grade Count:3 |
|
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..
|
|||