| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
|
ExxonMobil Bicor® 100 LTSC OPP Film
Product Description: Bicor LTSC is a two-side coated OPP film which is designed for use in high-speed or demanding horizontal, fin seal, packaging applications. The low-temperature seal coating (LTS..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
|
ExxonMobil Bicor® 220 AB OPP Film
Product Description: Bicor AB is a two-side acrylic coated, sealable OPP film designed for general use in overwrap and horizontal packaging. It can be surface printed, reverse printed, or used unpri..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
|
ExxonMobil Bicor® 30 ARW OPP Film
Product Description: Bicor ARW is a two-side acrylic coated OPP film designed for use in lamination and monoweb applications, especially for paper ream wrap. The acrylic-coated side with the higher ..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
|
ExxonMobil Bicor® 380 AB OPP Film
Product Description: Bicor AB is a two-side acrylic coated, sealable OPP film designed for general use in overwrap and horizontal packaging. This film is suitable as an unsupported web or lamination..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
|
ExxonMobil Bicor® 85 LTSC OPP Film
Product Description: Bicor LTSC is a two-side coated OPP film which is designed for use in high-speed or demanding horizontal, fin seal, packaging applications. The low-temperature seal coating (LTS..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
|
ExxonMobil Bicor™ 70 MB OPP Film
Product Description: Bicor 70 MB is a biaxially oriented polypropylene film for use in metalized film applications. 70 MB, when metalized, is used in adhesive and extrusion laminations to reveres-pr..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
|
ExxonMobil Label-Lyte® 18 LLG-101 Clear OPP Film
Product Description: A clear, one-side treated, polypropylene film that is designed to provide exceptional clarity and print protection when used as over laminates in pressure-sensitive labeling app..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | 510 |
|
ExxonMobil Label-Lyte® 612 LLG-102 Clear OPP Film
Clear, polypropylene films designed for use in roll-fed labeling applications. This film can be laminated to itself or applied as an outer web to other films. The print surface is a treated high ene..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
|
ExxonMobil Label-Lyte™ 18LL-101 OPP Film
Product Description: A clear, one-side treated, polypropylene film that is designed to provide exceptional clarity and print protection when used as overlaminates in pressure-sensitive labeling appl..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
|
ExxonMobil Label-Lyte™ 612LLG102 OPP Film
Product Description: A clear, two-side treated, polypropylene film that is used in roll-fed labeling applications. This film can be laminated to itself or applied as an outer web to other films. 612..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 054 Polyester Film
Melinex® 054 is a high clarity, low balanced shrink polyester film which is two-side pretreated to promote adhesion to industrial coatings and inks.Information provided by DuPont.
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 3381 Polyester Film
Melinex® 3381 is a two-side heat sealable, opaque white polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well a..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 359 Polyester Film, 500 Gauge
Melinex® 359 is a white opaque polyester film with a two side chemical pre-treatment for improved ink adhesion and laser printing.Information provided by DuPont.
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 359 Polyester Film, 700 Gauge
Melinex® 359 is a white opaque polyester film with a two side chemical pre-treatment for improved ink adhesion and laser printing.Information provided by DuPont.
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 565 Polyester Film
Melinex® 565 is a high clarity film which is differentially coated. One surface is coated with the standard T-Sub adhesion promoter; the opposite surface is coated for antistatic protection.Informa..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® ST339 Polyester Film, 1000 Gauge
Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® ST339 Polyester Film, 200 Gauge
Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® ST339 Polyester Film, 300 Gauge
Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® ST339 Polyester Film, 380 Gauge
Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® ST339 Polyester Film, 500 Gauge
Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® ST339 Polyester Film, 700 Gauge
Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® EB31 Polyester Film, 200 Gauge
Mylar® EB31 is a smooth, matte polyester film. It does not contain any plasticizers. General Product Info: Mylar® EB31 has low haze and intermediate gloss. This offers more realistic colors and cl..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® EB31 Polyester Film, 92 Gauge
Mylar® EB31 is a smooth, matte polyester film. It does not contain any plasticizers. General Product Info: Mylar® EB31 has low haze and intermediate gloss. This offers more realistic colors and cl..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ExxonMobil Method |
|
ExxonMobil Bicor® 110 ASB-X OPP Film
Product Description: Bicor ASB-X is a two side coated, sealable OPP film designed for broad use in many applications, including overwrap, horizontal, and vertical packaging. ASB-X is good for heavy ..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
|
ExxonMobil Bicor® 120 LTSC OPP Film
Product Description: Bicor LTSC is a two-side coated OPP film which is designed for use in high-speed or demanding horizontal, fin seal, packaging applications. The low-temperature seal coating (LTS..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
|
ExxonMobil Bicor™ 25 ARW OPP Film
Product Description: Bicor ARW is a two-side acrylic-coated OPP film designed for use in lamination and monoweb applications, especially for paper ream wrap. The acrylic-coated side with the higher ..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 523 Polyester Film
Melinex® 523 is a high clarity polyester film. It is pretreated on both surfaces with MAP (multiple application pretreatment) to promote adhesion to most aqueous and solvent coating formulations. I..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | ASTM D882 |
|
Honeywell MAP-Shield™ AF Generation 2 Shrinkable Barrier Film
(discontinued **)
Description: MAP-Shield™ AF shrinkable barrier film is ideal for modified atmosphere packaged (MAP) food products in barrier trays for extended shelf life protection. The coextruded, biaxially orie..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | 510 |
|
ExxonMobil Bicor® 120 LCX OPP Film
One-side treated, one-side sealable OPP film designed for use in a lamination. It is typically laminated to Metallyte, HBS-2, SPW, and itself to create lap sealable packages. The high energy surfac..
|
|||
| Film Tensile Strength at Break, MD | 138 MPa | 20000 psi | 510 |
|
ExxonMobil Label-Lyte® 612 LL-112 Clear OPP Overlaminate
Clear, polypropylene film designed to provide exceptional clarity and print protection when used as an overlaminate in pressure-sensitive labeling applications. The treated high energy layer provide..
|
|||