| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 437 Polyester Film, 200 Gauge
Melinex® 437 is a two side differentially pretreated super clear film; 1 side promotes adhesion, 1 side slip.Also available in 270, 370, 465, 650 GaugeInformation provided by DuPont.
|
|||
| Film Tensile Strength at Break, MD | >= 172 MPa | >= 25000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 461 Polyester Film
Melinex® 461 is a high clarity polyester film manufactured with a coating on one surface that promotes adhesion to many solvent formulations and to most vinyl or acrylic base ink systems. The adhes..
|
|||
| Film Tensile Strength at Break, MD | >= 172 MPa | >= 25000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 473 Polyester Film, 200 Gauge
Melinex® 473 is a high clarity polyester film manufactured with a coating on one surface that improves slip and handling characteristics. The opposite surface is raw polyester (non-coated). The sli..
|
|||
| Film Tensile Strength at Break, MD | >= 172 MPa | >= 25000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 478 Polyester Film, 200 Gauge
Melinex® 478 is a high clarity polyester film manufactured with a coating on both surfaces that improves slip and handling characteristicsTypical Applications: Melinex 478 is used in many general i..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 515 Polyester Film
A high clarity film which is two side pretreated for slip to combine good handling properties with high clarity and brilliance.Typical Applications: MELINEX® 515 is suitable for applications which ..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 623 Polyester Film, 750 Gauge
Melinex® 623 is a super clear polyester film pretreated on both surfaces to give superior solvent adhesion and improved handleability.Information provided by DuPont.
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 680 Polyester Film, 750 Gauge
Melinex® 680 is a super clear polyester film, pretreated on one side to promote adhesion with improved handleability. It is high clarity, non-yellow base with excellent adhesion on the pretreated s..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® WCW Polyester Film, 200 Gauge
Melinex® WCW is a translucent white polyester film with a rough surface for superior handling characteristics.Information provided by DuPont.
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® WCW Polyester Film, 92 Gauge
Melinex® WCW is a translucent white polyester film with a rough surface for superior handling characteristics.Information provided by DuPont.
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® E Polyester Film, 142 Gauge
Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® E Polyester Film, 200 Gauge
Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® E Polyester Film, 300 Gauge
Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® E Polyester Film, 92 Gauge
Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® M461 Polyester Film, 200 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® M461 Polyester Film, 48 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® M461 Polyester Film, 500 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® M461 Polyester Film, 60 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® OL2 Polyester Film, 100 Gauge
Product Description: Mylar® OL2 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sealable lidding film in packaging refrigerated and f..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® OL2 Polyester Film, 50 Gauge
Product Description: Mylar® OL2 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sealable lidding film in packaging refrigerated and f..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® OL2 Polyester Film, 75 Gauge
Product Description: Mylar® OL2 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sealable lidding film in packaging refrigerated and f..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® OWF2 Polyester Film, 60 Gauge
Product Description: Mylar® OWF2 is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. Mylar® OWF2 has a thicker heat sealable layer than Myla..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® RB42AF Polyester Film, 100 Gauge
Product Description: Mylar® RB42AF is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer and polyvinylidene chloride (PVdC) layer on the opposite side. ..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® RB43 Polyester Film, 100 Gauge
Mylar® RB43 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite side. Mylar® R..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® RB52 Polyester Film, 50 Gauge
Product Description: Mylar® RB52 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opp..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® RL31 Polyester Film, 100 Gauge
Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Myl..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® RL31 Polyester Film, 75 Gauge
Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Myl..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® RSX Polyester Film, 105 Gauge
Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® RSX Polyester Film, 400 Gauge
Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® M461 Polyester Film, 400 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..
|
|||
| Film Tensile Strength at Break, MD | 172 MPa | 25000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® RSX Polyester Film, 200 Gauge
Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust..
|
|||