| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Film Tensile Strength at Break, MD | 200 - 290 MPa | 29000 - 42000 psi | ASTM D882 |
|
Honeywell Capran® Oxyshield™ OEB (0.60 mil) Monoaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film
Description: Oxyshieldâ„¢ Oriented Extra Barrier is a 0.60 mil (15 micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of ..
|
|||
| Film Tensile Strength at Break, MD | 200 - 290 MPa | 29000 - 42000 psi | ASTM D882 |
|
Honeywell Capran® Oxyshield™ OEB (1.0 mil) Monoaxially Oriented, Co-Extruded Nylon6/EVOH/Nylon 6 Clear Film
Description: Oxyshieldâ„¢ Oriented Extra Barrier is a 1.00 (25micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relat..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | Orientation not specified; ASTM D882 |
|
DuPont™ Kapton® 250FN029 Polyimide/FEP Composite Film
250 Gauge film structure consisting of a 50 µm (2 mil) base polyimide film with a 13 µm (0.5 mil) coating of Teflon® FEP on one side.Kapton® Type HN film coated with Teflon® FEP fluoropolymer r..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 426 Polyester Film, 92 Gauge
Melinex® 426 is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. Melinex® 426 is chemically treated on one side for static control. The tre..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® 426P Polyester Film, 92 Gauge
Melinex® 426P is a slightly hazy film with excellent handling characteristics. Melinex® 426P is chemically treated on one side to minimize static charge. The treatment provides stable antistatic p..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® FRPS Polyester Film, 142 Gauge
Melinex® FRPS is a lower shrinkage version of Melinex® S. Designed specifically for release applications in the fiberglass reinforced panel industry, with consistently good cross-web flatness and ..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® S Polyester Film, 200 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® S Polyester Film, 300 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® S Polyester Film, 400 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® S Polyester Film, 500 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® S Polyester Film, 92 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882 |
|
DuPont Teijin Films Mylar® 75 OL Polyester Film, 75 Gauge
Data provided by DuPont Packaging Polymers.An exceptionally strong polyester film designed to package foods. The film is suitable for heating food products in microwave or conventional ovens. Can b..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® D804 Polyester Film, 92 Gauge
Mylar® D804 is a super clear, biaxially oriented, co-extruded polyester film, available in 60, 75 and 92 gauge. Mylar® D804 is two-side pretreated for printing and adhesive lamination. Approvals: ..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® HP Polyester Film, 48 Gauge
Mylar® HP film is a high strength, high clarity and low haze polyester film with dimensional stability particularly suitable for use in applications where dimensional stability is a requirement dur..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® HP Polyester Film, 60 Gauge
Mylar® HP film is a high strength, high clarity and low haze polyester film with dimensional stability particularly suitable for use in applications where dimensional stability is a requirement dur..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882 |
|
DuPont Teijin Films Mylar® LB Polyester Film, 75 Gauge (19 µm)
Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film designed for use as a component of a lamination. Standard thickness offered include 48, 75, and 92 gauges. Variet..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882 |
|
DuPont Teijin Films Mylar® LBT Polyester Film, 75 Gauge (19 µm)
Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film that has been corona-treated to provide superior wetting and adhesion to inks, primers, and adhesives. Standard th..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® LBTW Polyester Film, 75 Gauge
Mylar® LBTW is an uncoated, transparent polyester film that has been corona treated on one side to provide superior wetting and adhesion of inks, primers, and adhesives. Mylar® LBTW is commerciall..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Mylar® S1 Polyester Film, 35 Gauge
Mylar® S1 films are slightly hazy with surfaces tailored to provide excellent handling and product functionality for a variety of industrial end uses. The outstanding tensile properties and thermal..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Teijin® Tetoron® SL Polyester Film, 200 Gauge
Teijin® Tetoron® SL is a low shrinkage version of Teijin® Tetoron® type S polyester film. In addition to having the well balanced physical, chemical and electrical properties of type S film, Tei..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Teijin® Tetoron® SL Polyester Film, 300 Gauge
Teijin® Tetoron® SL is a low shrinkage version of Teijin® Tetoron® type S polyester film. In addition to having the well balanced physical, chemical and electrical properties of type S film, Tei..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Teijin® Tetoron® SLA Polyester Film, 200 Gauge
Teijin® Tetoron® SLA is a super low shrinkage version of Teijin® Tetoron® type S polyester film. In addition to having the well balanced physical, chemical and electrical properties of type S fi..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® S Polyester Film, 142 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Melinex® S Polyester Film, 75 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
|
|||
| Film Tensile Strength at Break, MD | 200 MPa | 29000 psi | ASTM D882A |
|
DuPont Teijin Films Teijin® Tetoron® SL Polyester Film, 500 Gauge
Teijin® Tetoron® SL is a low shrinkage version of Teijin® Tetoron® type S polyester film. In addition to having the well balanced physical, chemical and electrical properties of type S film, Tei..
|
|||