| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 0.862 - 41.4 MPa | 125 - 6000 psi | Average value: 20.5 MPa Grade Count:49 |
|
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..
|
|||
| Tensile Strength, Yield | 0.862 MPa | 125 psi | at 100%; ASTM D412 |
|
Multibase Multi-Flex® A 3005 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowFoamableHeat StabilizedGeneral PurposeOzone ResistantProce..
|
|||
| Tensile Strength, Yield | 0.862 MPa | 125 psi | ASTM D412 |
|
Saint-Gobain COHRlastic® R10450 Medium Fiberglass Reinforced Silicone Sponge Rubber
Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons..
|
|||
| Tensile Strength, Yield | 0.862 MPa | 125 psi | Transverse/Width |
|
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.004" thick)
Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-..
|
|||
| Tensile Strength, Yield | 0.862 MPa | 125 psi | Transverse/Width |
|
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.005" thick)
Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-..
|
|||
| Tensile Strength, Yield | 0.862 MPa | 125 psi | |
|
Master Bond Mastersil 713 Low Viscosity One Component Silicone
Master Sil 713 is a ready-to use, exceptionally low viscosity, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. This ..
|
|||