Polymer Property : Tensile Strength, Yield = 1.03 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.03 MPa
149 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Gravi-Tech™ GRV-TP-080-W-NAT Styrene Butadiene Block Copolymer (SBC)
Information provided by PolyOne
Tensile Strength, Yield 1.03 MPa
150 psi
TM R050-36
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin
Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (..
Tensile Strength, Yield 1.03 - 2900 MPa
150 - 420000 psi
Average value: 576 MPa Grade Count:102
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Yield 1.03 MPa
150 psi
at 200%, molded-without post cure; ASTM D412
Multibase C6-235 DI-CUP R Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield >= 1.03 MPa
>= 149 psi
Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7282 Neoprene / Chloroprene
UL-flame resistant, non-blooming neopreneInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 1.03 MPa
150 psi
Transverse/Width
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.006" thick)
Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-..
Tensile Strength, Yield 1.03 MPa
150 psi
Transverse/Width
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.008" thick)
Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-..
Tensile Strength, Yield 1.03 MPa
150 psi
Transverse/Width
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.010" thick)
Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-..
Tensile Strength, Yield 1.03 MPa

@Strain 300 %
150 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP 1107 Thermoplastic Elastomer
Notes: General Purpose; OpaqueInformation Provided by Teknor Apex
Tensile Strength, Yield 1.03 MPa

@Strain 300 %
150 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP 1736R Thermoplastic Elastomer
Notes: Soft Material; Overmold onto PP handlesInformation Provided by Teknor Apex
Tensile Strength, Yield 1.03 MPa
150 psi
at 150% elongation, maximum
Dow Corning SILASTIC® 94-595-HC SILICONE RUBBER PART A&B
30 Durometer, 2-part, 1 to 1 mix, translucent, Injection Moulding grade, Liquid Silicone Rubber.Information provided by Dow Corning
Tensile Strength, Yield 1.03 MPa
150 psi
Resinlab® UR3005 Clear Two Part Urethane Elastomer
Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi..
Tensile Strength, Yield 1.03 MPa
150 psi
Resinlab® UR3005 Two Part Urethane Elastomer
Resinlab™ UR 3005 is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 provides excellen..
Tensile Strength, Yield 1.03 MPa
150 psi
AVG Stress at Elongation M25; ASTM D412 Method A
Seals Eastern 5861 Fluoro-silicone
Fluoro-silicone meeting MIL-R-25988BInformation provided by Seals Eastern, Inc.