| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | ASTM D638 |
|
Nylene® 406F Nylon 6
Dry as molded. Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling..
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | ASTM D638 |
|
Nylene® 409 Nylon 6
Dry as molded. Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles..
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | 50 mm/min; ISO 527-1,2 |
|
Qualchem Danamid FEHUV Polyamide 6
Heat and UV stabilized, for long-lasting use at 120-130°C, protected against artificial lightInformation provided by Qualchem Zrt.
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | |
|
Radici Radilon® A ERV1906LK (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 527-1/2 |
|
Radici Radilon® CST (dry) Copolyamide 6 semiaromatic
Transparent gradeInformation provided by Radici group.
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 5271/2 |
|
Radici Radilon® S 35FL (dry) Nylon 6
Radilon® S (homopolyamides) are normally used in cast and blown extrusion for the production of packaging films. Radilon® S grades can be extruded to a thickness varying from 20 mm to 100 mm.Appl..
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 527-1/2 |
|
Radici Radilon® S35HR (dry) Nylon 6
Medium high viscosityInformation provided by Radici group.
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 527-1/2 |
|
Radici Radilon® S40E (dry) Nylon 6
High viscosity for extrusionInformation provided by Radici group.
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 527 |
|
SABIC Innovative Plastics LNP COLORCOMP R1000S PA 66
LNP COLORCOMP* R1000S is an unfilled Nylon 66. Added features of this material is: Heat Stabilized.
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific)
Transparent Polycarbonate in natural color. Excellent processability, super high flow.
|
|||
| Tensile Strength, Yield |
75.0
MPa <br>@Temperature 22.0 °C
|
10900
psi <br>@Temperature 71.6 °F
|
25mm flat samples, compression moulded; ISO 527-4 |
|
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP
SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond..
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 527-1/-2 |
|
Lanxess Durethan® B 40 FKA 000000 Nylon 6, Film Grade
PA 6 film grade of high viscosity, nucleated and lubricated, in compliance with FDA for food contactApplication Examples: flat and blown film, flat film coextrusion for PA/PE composite films
|
|||
| Tensile Strength, Yield |
75.0
MPa <br>@Temperature 22.0 °C
|
10900
psi <br>@Temperature 71.6 °F
|
25mm flat samples, compression moulded; ISO 527-4 |
|
Menzolit Menzolit® SMC 0420 Unsaturated Polyester UP
SMC 0420 is a low density Premium Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to light weight parts with good up to excellent surface quality for ..
|
|||
| Tensile Strength, Yield |
75.0
MPa <br>@Temperature 22.0 °C
|
10900
psi <br>@Temperature 71.6 °F
|
25mm flat samples, compression moulded; ISO 527-4 |
|
Menzolit Menzolit® SMC 0421 Unsaturated Polyester UP
SMC 0421 is a low density premium Class-A SMC for on-line painted exterior body applications on cars. These compounds mould to light weight parts with excellent surface quality for on-line painted ..
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP JZL012 PES (Europe-Africa-Middle East)
LNP* LUBRICOMP* JZL012 is a compound based on Polyethersulfone resin containing Proprietary Filler, PTFE. Added features include: Internally Lubricated.
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Valox® 4012G PBT
VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP DF0029R PC (Europe-Africa-Middle East)
LNP* Thermocomp* DF0029R is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Mold Release, Flame Retardant.
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Noryl GTX VP7133 PPE+PA (Europe-Africa-Middle East)
Noryl GTX VP7133 is an unfilled extrusion grade which offers high heat resistance in combination with high meltstrength.The material is especially designed for thermal break profiles which are used ..
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 527-2 |
|
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced
GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi..
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | ASTM-D638 |
|
Polyram PlusTek PA517 Nylon 6.6, Flame Retardant
Flame retardant halogen free polyamide 6.6 formulated to meet V-0, for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 527-2 |
|
Tisan TISLAMID® 6 30% Mineral Reinforced Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 527-2 |
|
Tisan TISLAMID® 6 Flame Retardant (V0) Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | |
|
Hexcel® HexPly® F263 Epoxy Resin
HexPly® F263 is a structural, heat resistant epoxy resin formulated for excellent translation of high modulus carbon fiber properties in typically aerospace applications. HexPly® F263 is a high te..
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | dry; ISO 527 |
|
Ter Hell Plastic Terez® PA 6.6 7750 T Polyamide 66
Description: Dry impact unfilled Polyamide 6.6, good flowability and demolding properties.Application: Molding parts of different kinds, high impact properties.Information provided by Ter Hell Plas..
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 527-1/-2 |
|
DuPont Performance Polymers Delrin® PC691 NC010 Acetal (POM)
(Unverified Data**)
Nucleated Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC690 is a low viscosity acetal homopolymer developed for parts requiring high precision molding in the health..
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | dry; ISO 527-1/-2 |
|
EMS-Grivory Grivory® TR 55 PA12/MACMI
Product description: Grilamid TR 55 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 55 natural offers outstanding properties..
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO R 527 |
|
Addiplast Addinyl B2 E Flame Retardant Nylon 6
Flame retardant, halogen freeInformation provided by Addiplast.
|
|||
| Tensile Strength, Yield | 75.0 MPa | 10900 psi | |
|
Asahi Kasei Xyron® G701H Modified Polyphenylene Ether
Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P..
|
|||
| Tensile Strength, Yield | 75.0 - 110 MPa | 10900 - 16000 psi | Average value: 93.5 MPa Grade Count:6 |
|
Overview of materials for Polyphenylene Ether, Glass/Graphite Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Glass/Graphite Reinforced". Each property range of values reported is minimum and m..
|
|||