| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
|
Oxford Polymers Oxnilon 66-13GF 13% Glass Fiber Filled Nylon 66 for Injection Molding
13% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
|
Ravago Manufacturing Americas Hylex® P1310G20 HB Polycarbonate, 20% Fiberglass Reinforced, UV Stabilized
Information provided by Ravago.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
|
Ravago Manufacturing Americas Hylex® P1010G20 HB Polycarbonate, 20% Fiberglass Reinforced
Information provided by Ravago.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
|
Gharda Chemicals Gafone S S1430SP60 Polysulfone (PS)
(discontinued **)
Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec..
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
|
Kostat 1940 Conductive PC Compound
KOSTAT 1940 is a conductive thermoplastic compound based on Polycarbonate and a special carbon fiber. KOSTAT 1940 is not dependant on atmospheric conditions and is used for ESD injection molded pro..
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
|
LG Chemical Lupox® GP-2151F General Purpose PBT, 15% Glass Fiber Reinforced, Flame Retardant
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics ULTEM 1000F PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 Listing. Effective June, 2007 this grade will no long..
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Ultem 1010A PEI (Europe-Africa-Middle East)
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics ULTEM 1010F PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer be ..
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Ultem 1010FV PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa..
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Ultem 1010V PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa..
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Ultem 1010V PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa..
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Ultem 1100R PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics ULTEM 1110F PEI (Europe-Africa-Middle East)
Enhanced flow PolyetherimiEnhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no long..
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics Ultem 1110R PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics ULTEM 9011 PEI (Europe-Africa-Middle East)
Transparent, high flow Polyetherimide (Tg 217C). Resin is RoHS compliant. Improved processability for Fiber extrusion.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics ULTEM HU1100 PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Ultem MD130A PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
|
SPS Guang Zhou POBUXâ„¢ 3001G15 Flame-retarded/GF15%-PBT
Characteristic: Good flame retardance, high mechanical properties, high rigidity, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) ..
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
|
Techmer ES HiFill® POM CO GF25 CC 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 25% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Ultem 1010KM PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics Valox® SHF4960 PBT
Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific)
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable..
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM-D638 |
|
Polyram PlusTek PA320G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant
25% glass fiber reinforced, flame retardant and high stiffness polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM-D638 |
|
Polyram PlusTek PB305G33 Nylon 6, 33% Glass Fiber
33% glass fiber reinforced, heat stabilized and UV stabilized polyamide 6 approved and listed by W.R.C and NSF/ANSI 61 international for potable waterInformation provided by Polyram Ram On Ind.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
|
Westlake Plastics Pomalux® 25% GF Acetal Copolymer 25% Glass Filled
Pomalux is a high performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even when machining par..
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM-D638 |
|
Polyram RamTough RZ310G6 Polycarbonate, 30% Glass Fiber
30% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | GB-1040 |
|
Zhejiang Juner PA-A6 GF20%
Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
|
|||
| Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM-D638 |
|
Polyram PlusTek PB321I6 Nylon 6, 30% Glass Fiber and Mineral
30% glass fiber and mineral reinforced polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||