| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
|
PolyOne LubriOne™ NL-30GF/15T Black Polyamide 612 (Nylon 612)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5.1 mm/min; ASTM D638 |
|
PolyOne Stat-Tech™ OC-0307081 Black Acrylonitrile Butadiene Styrene + PC (ABS+PC)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
|
|||
| Tensile Strength, Yield |
119
MPa @Temperature 100 °C |
17300
psi @Temperature 212 °F |
ISO 527 |
|
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d
AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, ..
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI
LNP* LUBRICOMP* EX06405 is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible, Easy Molding.
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI (Asia Pacific)
LNP* Lubricomp* EX06405 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66
LNP* LUBRICOMP* RFL33 is a compound based on Nylon 66 resin containing 15% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Asia Pacific)
LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics ULTEM 2110EPR PEI
10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific)
10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | ISO 527 |
|
SABIC Innovative Plastics LNP STAT-KON DE0039 PC
LNP* STAT-KON* DE0039 is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Flame Retardant. Electrically Conductive.
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
|
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific)
LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
|
|||
| Tensile Strength, Yield | 119 MPa | 17200 psi | ASTM D638 |
|
Techmer ES HiFill® PA4/6 M/GF 20 HS 20% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 119 MPa | 17200 psi | ASTM D638 |
|
Techmer ES HiFill® PA6 GF/B30 HS L BK 30% Glass Fiber/Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 30% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: ..
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
|
Techmer ES HiFill® PA6 GF/M40 HS L BK 40% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackProc..
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
|
Techmer ES HiFill® PA6 GF/M40 IG BK 40% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedProcessing Method: In..
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP THERMOCOMP DF006RXQ PC
LNP* THERMOCOMP* DF006RXQ is a compound based on Polycarbonate resin containing 30% Glass Fiber.
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS
Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific)
Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | ISO 527 |
|
SABIC Innovative Plastics LNP STAT-KON DE0039 PC (Asia Pacific)
LNP* Stat-kon* DE0039 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Flame Retardant.
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
|
SABIC Innovative Plastics LNP STAT-KON DX06500 PC
LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy ..
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | SABIC - Japan Method |
|
SABIC Innovative Plastics NORYL CN5258 PPE+PS (Asia Pacific)
40% filled FR high modulus PPE/PS blend
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East)
Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
|
Ensinger Tecapeek® PVX Polyetheretherketone (PEEK)
TECAPEEK® PVX is an ultra high performance bearing material made from Victrex® PEEK polymer. TECAPEEK® PVX incorporates the properties of a premium polymetric matrix material with optimum levels..
|
|||
| Tensile Strength, Yield |
119
MPa @Temperature -40.0 °C |
17300
psi @Temperature -40.0 °F |
ISO Data |
|
BASF Ultramid® 8270 HS PA6 (Conditioned)
Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi..
|
|||
| Tensile Strength, Yield |
119
MPa @Temperature -40.0 °C |
17300
psi @Temperature -40.0 °F |
ASTM Test |
|
BASF Ultramid® 8270 HS PA6 (Conditioned)
Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi..
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
|
Omni Plastics OmniLon™ 6/6 PA6/6 GR20 IM10 Glass Reinforced/Impact Modified Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
|
Custom Resins Vexel™ 4200 RD PBT; 30% Glass Filler
(discontinued **)
Property data for dry as molded samples.Data provided by the manufacturer
|
|||
| Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP STAT-KON QEP35M PA6.10
LNP STAT-KON QEP35M is a compound based on Nylon 6/10 resin containing 25% Milled Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Electrically Conductive, Wear Resistant.
|
|||