| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | Type 1B, 50mm/min; ISO 527-1/2:1993 |
|
Nylacast Nylube MO Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), MoS2 Filled
The combined Nylube lubrication system incorporating fine particles of molybdenum disulphide provides enhanced load bearing capabilities while retaining Nylube's excellent frictional characteristics..
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS
PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance.
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | |
|
Radici Radilon® S RCV3015 (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
|
|||
| Tensile Strength, Yield | 84.8 MPa | 12300 psi | ASTM D638 |
|
LNP Lubricomp® PDX-E-00548 CCS Polyetherimide, Aramid Fiber Reinforced, PTFE Lubricant
(discontinued **)
Features: Lubricated, Low to None Ion ContentForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however man..
|
|||
| Tensile Strength, Yield |
85.0
MPa <br>@Temperature 23.0 °C
|
12300
psi <br>@Temperature 73.4 °F
|
DAM; ISO 527 |
|
DuPont Performance Polymers Zytel® 103FHS BKB038 Nylon 66
(Unverified Data**)
Zytel® 103FHS BKB038 is a heat stabilized, lubricated, PA 66 resin for fast cycling.Information provided by DuPont Performance Polymers
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | ASTM value at 50 mm/min. |
|
BASF Capron® 5202 HS BK-102 Nylon 66 (Dry)
(discontinued **)
Capron 5202 HS BK-102 is an unfilled, heat stabilized, pigmented black nylon 6,6, injection molding compound. It combines strength and stiffness as well as excellent chemical resistance. The additi..
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527-1/-2 |
|
Lanxess Durethan® B 31 SK 000000 Nylon 6
PA 6, injection molding grade, non-reinforced, easy flow, easy-release, rapid solidification, crystallizes somewhat more finely and uniformly than B 30 S
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527-1/-2 |
|
Lanxess Durethan® A 30 000000 Nylon 66
PA 66, standard injection molding grade, non-reinforced, very easy release, normal solidificationApplication Examples: terminal blocks, cable clips, bobbins, gearwheels
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | d.a.m.; ISO 527-1, -2; 50 mm/min |
|
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant
PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS.
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527 type 1 A |
|
Solvay TECHNYL® C 206 PA6, DRY
Description: Unreinforced Polyamide PA6, standard for fast cycling, for injection molding.Available in: EuropeProduct Applications: TECHNYL® C 206 has fluidity and a good mould release, favored b..
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East)
VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin.
|
|||
| Tensile Strength, Yield | 84.8 MPa | 12300 psi | ASTM D638 |
|
Techmer ES Luriblend® PA6/6 T/AL20 HS 10% Aramid Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid Fiber, 10% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated, Heat Stabilized, Low Friction ..
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East)
Super high flow FR PBT grade with 15% Glass reinforced
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | ASTM-D638 |
|
Polyram PA500 Nylon 6.6, Flame Retardant
Flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | ASTM-D638 |
|
Polyram PlusTek PB140 Nylon 6, Injection Molding
Polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | dry; ISO 527-1/-2 |
|
DSM Akulon® F160-Z PA6
Very High Viscosity, Lubricated
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527-1/-2 |
|
DSM Akulon® F223-D (Dry) Low/Medium Viscosity Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | dry; ISO 527-1/-2 |
|
DSM Akulon® F-X9183 PA6
Low/Medium Viscosity
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | 50 mm/min; ISO 527 |
|
Eurostar Staramide A28 PA66, Injection Molding
Staramide A28 is an Unreinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | ASTM D638 |
|
E-Polymers TEKANATE™ G730 , 30% Glass Fiber Reinforced Poly Carbonate
30% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd.
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | DAM; ISO 527-1/-2 |
|
DuPont Performance Polymers Zytel® 103FHS BKB038 Nylon 66
(Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS BKB038 is a heat stabilized lubricated PA 66 resin for fast cycling.Information provided by DuPont Performance Polymers
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | DAM; ISO 527-1/-2 |
|
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527-2 |
|
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | 50mm/min; ISO 527 |
|
BASF Ultramid® 1003-2 NF2002 PA66 (Dry)
Ultramid 1003-2 NF2002 is a general purpose, heat stabilized nylon 6/6.
|
|||
| Tensile Strength, Yield |
85.0
MPa <br>@Temperature 20.0 °C
|
12300
psi <br>@Temperature 68.0 °F
|
|
|
BASF Ultrason E 3010 PES
Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance.
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527-1/-2 |
|
DSM Stanyl® TE350 Nylon 46 (European and Asian Grade) (Dry)
(discontinued **)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | DAM; ISO 527-1/-2 |
|
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66
(Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS BKB009 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productiv..
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | 50 mm/min |
|
Arkema Group Oroglas® V 825 T Acrylic
(discontinued **)
OROGLAS V 825 T exhibits an excellent balance of properties including superior thermal resistance with an easy processing behavior.OROGLAS V 825 T is then the material of choice for automotive appli..
|
|||
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527 |
|
BASF Ultramid® A3K Q601 PA66(Dry)
Description: Ultramid A3K Q601 is an easy flowing, injection molding grade PA66.Applications: Typical applications include fast processing high stress technical parts or electrically insulating part..
|
|||