| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | 50 mm/min; ASTM D638 |
|
Ovation Polymers OpteSTAT™ NC PES 6010 Polyether Sulfone based Carbon Nanotube Compound
Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or..
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC
LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing 30% Mixed Glass, 15% PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Tensile Strength, Yield |
90.0
MPa <br>@Temperature 22.0 °C
|
13100
psi <br>@Temperature 71.6 °F
|
25mm flat samples, compression moulded; ISO 527-4 |
|
Menzolit Menzolit® SMC 0400 Unsaturated Polyester UP
SMC 0400 is a Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to parts with good up to excellent surface quality for medium bake in-line and off-line p..
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | ISO 527-1/-2 |
|
Lanxess Durethan® A 30 H2.0 901510 Nylon 66
PA 66 standard injection molding grade, non-reinforced, very easy release, good heat-ageing resistanceApplication Examples: terminal blocks, cable clips, bobbins, gearwheels
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | ISO 527-1/-2 |
|
Lanxess Durethan® B 30 S FN40 000000 Nylon 6
PA 6, injection molding grade, non- reinforced, good flowability, easy-release, fast cycling, UL 94V-2 off 0,75 mm, GWIT 775°C bei 0,75/1,5mm
|
|||
| Tensile Strength, Yield |
90.0
MPa <br>@Temperature 22.0 °C
|
13100
psi <br>@Temperature 71.6 °F
|
25mm flat samples, compression moulded; ISO 527-4 |
|
Menzolit Menzolit® SMC 0412 Unsaturated Polyester UP
SMC 0412 is a premium Class-A SMC for on-line painted conductive exterior body applications on cars. These compounds mould to parts with excellent surface quality and low surface conductivity for e..
|
|||
| Tensile Strength, Yield |
90.0
MPa <br>@Strain 0.200 %,<br> Temperature 980 °C
|
13100
psi <br>@Strain 0.200 %,<br> Temperature 1800 °F
|
|
|
Haynes 718 alloy, cold rolled, solution-treated and aged sheet
Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i..
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As..
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics ULTEM 9075 PEI (Europe-Africa-Middle East)
High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution.
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East)
High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..
|
|||
| Tensile Strength, Yield |
90.0
MPa <br>@Strain 0.200 %
|
13100
psi <br>@Strain 0.200 %
|
Annealed |
|
Special Metals Nickel 205
Wrought nickel similar to Nickel 200 but with compositional adjustments to enhance performance in electrical and electronic applications. Ferromagnetic. Used for the anodes and grids of electronic..
|
|||
| Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
|
Techmer ES Plastiblend® PA6 L N BK002 Nylon 6
Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and Lubricant(4500 ppm)Features: Fast Molding Cycle, Good Processability, Nucleated and LubricatedAppearance: BlackTPCI# 1327102In..
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | ISO 527 type 1 A |
|
Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, Conditioned
Description: Polyamide PA66, reinforced with 15% of glass fiber, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 216 V15 is used in all sectors of industry, offer..
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | ISO 527 |
|
Polyram PlusTek PA201 Nylon 66 for Extrusion
High viscosity Nylon 66 for extrusion applications.Information provided by Polyram.
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | ASTM-D638 |
|
Polyram PlusTek PB150 Nylon 6, Injection Molding
Fast cycle polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | ISO 527 |
|
Polyram Polytron P20B11 Polypropylene, 20% Long Fiber Glass
A chemically coupled 20% long fiber glass reinforced black polypropylene, heat stabilized for injection molding applications.Information provided by Polyram.
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | ASTM-D638 |
|
Polyram RamTough RZ300G3 Polycarbonate, 15% Glass Fiber
15% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | ASTM D638 |
|
Cresset Powers Cress-Alon™ NF3020 2% Nano Clay Loaded, 3.0 r.v. Film Grade Nylon 6, 50% RH
Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib..
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® TSG-25/4 PA666-GF25
Information provided by EMS Grivory
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | dry; ISO 527-1/-2 |
|
EMS-Grivory Grivory® BS V0 PA6
Product description: Grilon BS V0 is an unreinforced, normal viscosity, self-extinguishing PA6 injection molding grade. Grilon BS V0 has the following important properties: Halogen and phosphorous-f..
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | ISO 527 |
|
Eurotec® Tecomid® NT40 NL PPA, unfilled, natural
Information provided by Eurotec®
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | 50mm/min; ISO 527 |
|
BASF Ultramid® 1310-11 NF2001 PA66 (Dry)
Ultramid 1310-11 NF2001 is a controlled crystallization, fast cycling PA6/6 which provides extremely fast cycle times and improved productivity over Ultramid 1000.
|
|||
| Tensile Strength, Yield |
90.0
MPa <br>@Temperature -40.0 °C
|
13100
psi <br>@Temperature -40.0 °F
|
ISO Data |
|
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Conditioned)
Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c..
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | 50 mm/min; ISO 527-1/-2 |
|
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Conditioned)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | 50 mm/min; ISO 527-1/-2 |
|
BASF Ultramid® KR 4350 PA6/6T (Conditioned)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | 50mm/min; ISO 527 |
|
BASF Ultramid® B27 E 01 PA6 (Dry)
Ultramid B27 E 01 is a low viscosity general-purpose, extrusion PA6 grade well suited for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German..
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | ASTM D638 |
|
Gharda Chemicals GATONE™ 5600PF Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® 3412ECR PC
Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v..
|
|||