| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL34 PC
LNP LUBRICOMP* DFL34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL34H PC
LNP LUBRICOMP* DFL34H is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Healthcare.
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | ASTM D638 |
|
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)
(Unverified Data**)
EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491°F), E..
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | 10%/min. ASTM D638 |
|
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **)
27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas ..
|
|||
| Tensile Strength, Yield | 93.79 MPa | 13600 psi | ASTM D638 |
|
Lucent Polymers GPCB-120 Polycarbonate+PBT, 20% Glass Fiber Reinforced
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics ULTEM 2312EPR PEI
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | Type I, 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | ASTM D638 |
|
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)
EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491..
|
|||
| Tensile Strength, Yield | 93.8 MPa | 13600 psi | ASTM D638 |
|
Techmer ES HiFill® ABS GF15 BK 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | SABIC - Japan Method |
|
SABIC Innovative Plastics Valox® AB9515 ABS+PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Tensile Strength, Yield | 93.8 MPa | 13600 psi | ASTM D638 |
|
Techmer ES HiFill® PA6/6 CM40 40% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: Natural ..
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6
LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity.
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6
4.0 specific gravity, Nylon 6
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOTUF VF004S SUPER TOUGH NYLON (Europe-Africa-Middle East)
LNP* THERMOTUF* VF004S is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS
Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Strength, Yield | 93.8 MPa | 13600 psi | ASTM D638 |
|
Techmer ES HiFill® ABS GF20 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 93.8 MPa | 13600 psi | ASTM D638 |
|
Techmer ES HiFill® ABS GF20 LE 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP Thermocomp GX05053 PSU (Europe-Africa-Middle East)
LNP* THERMOCOMP* GX05053 is a compound based on Polysulfone blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | ISO 527-2 |
|
Tisan TISOPLEN® 30% Glass Fiber Filled Reinforced Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Tensile Strength, Yield |
94.0
MPa @Temperature 23.0 °C |
13600
psi @Temperature 73.4 °F |
|
|
Hexcel® HexPly® 954-6 Curing Cyanate Resin
HexPly® 954-6 is a 250°F (121°C) curing toughened cyanate resin with 300°F (149°C) Tg. HexPly® 954-6 is formulated for autoclave curing. Recommended cure is three hours at 250°F (121°C). Ser..
|
|||
| Tensile Strength, Yield |
94.0
MPa @Temperature 23.0 °C |
13600
psi @Temperature 73.4 °F |
EN ISO 527 |
|
Ensinger TECASINT 5051 Polyimide, 30% Glass Fiber Filled (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | 5 mm/min; ISO 527 |
|
Eurostar Starflam RF023P PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam RF0023P is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding (also known as Starflam PA66C U2 Z23)Information provided by Eurostar.
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | |
|
Asahi Kasei Xyron® G702H Modified Polyphenylene Ether
Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P..
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | 2 in/min; ASTM Test |
|
BASF Ultramid® 1310-11 NF2001 PA66 (Dry)
Ultramid 1310-11 NF2001 is a controlled crystallization, fast cycling PA6/6 which provides extremely fast cycle times and improved productivity over Ultramid 1000.
|
|||
| Tensile Strength, Yield | 93.8 MPa | 13600 psi | ASTM D638 |
|
Asahi Kasei Thermylene® P6-30FG-0632 30% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | |
|
Asahi Kasei Xyron® G702V Modified Polyphenylene Ether
Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P..
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | 5 mm/min; ISO 527 |
|
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP JF004L PES
LNP* THERMOCOMP* JF004L is a compound is based on Polyethersulfone containing 20% Glass Fiber. Characteristics of this grade is: Low Extractible
|
|||
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | ISO 527-1/-2 |
|
Lanxess Durethan® DP 2801 000000 Nylon 66
PA 66 injection molding grade, non-reinforced, UL 94V-2 off 0,75 mm (listed), GWFI: 960°C off 0.75 mm, GWIT: 775°C off 0,75 mm, halogen-free
|
|||