Mechanical Properties Metric English Comments
Tensile Strength, Yield 121 MPa
17500 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Nymax™ GMF 604 40 UV Black 148 Polyamide 6 (Nylon 6)
The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor..
Tensile Strength, Yield 121 MPa
17500 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Nymax™ X GMF 604 40 UV Black 148 rev 4 Polyamide 6 (Nylon 6)
The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor..
Tensile Strength, Yield 121 MPa
17500 psi
ASTM Data
Dow Questra® QA802 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **)
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve..
Tensile Strength, Yield 121 MPa
17500 psi
ASTM Data
Dow Questra® WA205 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **)
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve..
Tensile Strength, Yield 121 MPa
17500 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
PolyOne Edgetek® PF-30GF/000 Polysulfone, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Yield 121 MPa

@Thickness 3.20 mm
17500 psi

@Thickness 0.126 in
ASTM D638
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE
NSF Certified for KA02 and E2035. Noted for High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts with water co..
Tensile Strength, Yield 121 MPa
17500 psi
ISO 527
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12
LNP* LUBRICOMP* IFL34 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Tensile Strength, Yield 121 MPa
17500 psi
ISO 527
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12 (Asia Pacific)
LNP* Lubricomp* IFL34 is a compound based on Nylon 6/12 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Tensile Strength, Yield 121 MPa
17500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP WFL34H PBT
LNP LUBRICOMP* WFL34H is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Healthcare.
Tensile Strength, Yield 121 MPa
17500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming.
Tensile Strength, Yield 121 MPa
17500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Asia Pacific)
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming.
Tensile Strength, Yield 121 MPa
17500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Europe-Africa-Middle East)
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. RoHS compliant.
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly (Asia Pacific)
LNP* Stat-kon* KE004 is a compound based on Acetal Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Techmer ES HiFill® PA6/6 GF18 FR BK 18% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 18% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Techmer ES HiFill® PC GF40 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc.
Tensile Strength, Yield 121 MPa
17500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DF004XXC PC (Europe-Africa-Middle East)
Polycarbonate compound, countaining Glass Fiber
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Techmer ES Luriblend® PC GF30 TL15 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: LubricatedInformation provided by TP Composites, Inc.
Tensile Strength, Yield 121 MPa
17500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp PFB139E PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PFB139E is a compound based on PA 6 resin containing Glass Fiber, Glass Bead, Flame Retardant. Added features include; Flame Retardant, Easy Molding.This data was supplied by SABIC-..
Tensile Strength, Yield 121 MPa
17500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp RF004S PA 66
LNP* Thermocomp* RF004S is a Nylon 6/6 containing Glass Fiber. Characteristics are Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength, Yield 121 MPa
17500 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12
LNP* THERMOCOMP* SF00A is a compound based on Nylon 12 resin containing 50% Glass Fiber.
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Techmer ES Electrablend® PA6/6 03001 Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Impact Modifier and Heat StabilizerFeatures: Electrically Conductive, Impact Modified and Heat Stab..
Tensile Strength, Yield 121 MPa
17500 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 (Asia Pacific)
Glass filled Nylon 12
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Westlake Plastics Norylux™ Modified Polyphenylene Oxide 30% glass filled
Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most d..
Tensile Strength, Yield 121 MPa
17500 psi
TriStar Ultracomp UC-300 Composite Bearing
Ultracomp UC-300 - Similar in construction to UC-200. Containing special fillers that reduce its coefficient of friction, UC-300 is designed to handle higher rotational and linear speeds.This family..
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D648
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
Tensile Strength, Yield 121 MPa
17500 psi
5 mm/min; ISO 527
Eurostar Starflam PFB139E PA6, Glass Fiber/Bead Filled, Flame Retardant, Injection Molded
Starflam PFB139E is a Flame Retardant Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding Resin (also known as PFB1013Z590)Information provided by Eurostar.
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Asahi Kasei Thermylene® P7-45FG-0790 45% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Omni Plastics OmniLon™ 6/6 PA6/6 GR15 Glass Reinforced Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Techmer ES HiFill® SPS GF40 BK 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: SyndiotacticAppearance: BlackInformation provided by TP Composites, Inc.