Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 19.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.3 MPa
2800 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable JC156HN Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Tensile Strength, Yield 19.3 MPa
2800 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable WJLK61 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Tensile Strength, Yield 19.3 MPa
2800 psi
Resinlab® CYNERGY CA6101 Adhesive
Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates..
Tensile Strength, Yield 19.3 MPa
2800 psi
Resinlab® CYNERGY CA6103 Adhesive
Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates..
Tensile Strength, Yield 19.3 MPa
2800 psi
Resinlab® CYNERGY CA6104 Adhesive
Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates..
Tensile Strength, Yield 19.3 MPa
2800 psi
Resinlab® CYNERGY CA6211 Adhesive
Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP..
Tensile Strength, Yield 19.3 MPa
2800 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Atomite Whiting Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 19.3 MPa
2800 psi
Resinlab® CYNERGY CA6203 Adhesive
Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP..
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D638
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Tensile Strength, Yield 19.3 MPa
2800 psi
2 in/min; ASTM D638
Ineos K38-20-188 HDPE
K38-20-188 is a natural, UV stabilized, medium density polyethylene resin designed specifically for use with an approved Ineos North America yellow masterbatch to produce pipe or tubing for natural ..
Tensile Strength, Yield 19.3 MPa
2800 psi
2 in/min (50 mm/min); ASTM D638
Ineos K38-20X2091 HDPE
K38-20X2091 is a yellow medium density polyethylene resin designed specifically for natural gas pipe extrusion. It exhibits excellent long term stress life and slow crack growth resistance. This m..
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D638
LyondellBasell Hifaxâ„¢ HSBMR246 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ HSBMR246 medium high melt flow, 1,500 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an outstanding balance of physical pro..
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D638
Spartech PP7230 Calcium Carbonate Filled High Impact Copolymer
Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by..
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D638
Techmer ES Statiblend® 02010 MB Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinfor.Features: ConductiveAppearance: BlackTPCI# 9125116Information provided by TP Composites, Inc.
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D412
Teknor Apex APEX® 90-A41R-85-NT Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by..
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D638
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle..
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D638
Westlake Plastics HIPS High Impact Polystyrene, Compression Molded
Compression molded HIPS is a low cost plastic material that is easily machined and fabricated. It is frequently used for preproduction prototyping. HIPS is a FDA compliant use in food processing a..
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D638
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle..
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D638
Total PSI 844E Polystyrene
Polystyrene 844E is a high impact polystyrene specially designed for the custom sheet market. The polymer produces tough ductile sheet with a rich matte finish. 844E is specially formulated to minim..
Tensile Strength, Yield 19.3 MPa
2800 psi
46% Ret.
UBE UBESTA® 3030U Nylon 12 (After Trichloroethylene for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Tensile Strength, Yield 19.3 MPa
2800 psi
Type IV; 50 mm per min; ASTM D638
Chevron Phillips Marlex® HHM TR-418Q MDPE Hexene Copolymer
High performance MDPE resin has been formulated for the demanding requirements of pressure pipe applications. Meets ASTM D4976 PE 225. Meets FDA Regulation 177.1520, suitable for food packaging ap..
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D638
ExxonMobil Paxon™ 7003 Crosslinkable Rotational Molding Resin
Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite..
Tensile Strength, Yield 19.3 MPa
2800 psi
Dow HDPE 04452N High Density Polyethylene
DOW HDPE 04452N resin is a narrow molecular weight distribution copolymer designed to offer good stress crack resistance and stacking strength with excellent impact strength. This resin has moderate..
Tensile Strength, Yield 19.3 MPa
2800 psi
50 mm/min cross speed; ASTM D638
DuPont™ Surlyn® 7930 Ionomer Resin, Lithium
Surlyn® 7930 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne..
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D-638
Axiall 11863 Wire & Cable Flexible PVC
Clear, UV resistant speaker wire.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D-638
Axiall 12881 Wire & Cable Flexible PVC
Flame retardant, specialty grade, 75°C rated jacket compound. Designed to present a unique clear, sparkling appearance to the finished cable.Information provided by Georgia GulfGeorgia Gulf became..
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D-638
Axiall 16881 Coax & Telecom Flexible PVC
90C rated, non-lead stabilized jacket compound with excellent low temperature properties. Suitable for riser and optical fiber constructions.Information provided by Georgia GulfGeorgia Gulf became ..
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D-638
Axiall 19482 Wire & Cable Flexible PVC
105°C, VW-1 rated non-lead stabilized insulation compound. Ideally suited for 18 AWG, 1/64 wall. UL approved for TW, THW, THHW applications.Information provided by Georgia GulfGeorgia Gulf became..
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D-638
Axiall 1055 Wire & Cable Flexible PVC
NM-B and UF-B jacket with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 19.3 MPa
2800 psi
2.0 in/min; ASTM D638
LTL Color Compounds ColorFast® FRPS100 Styrene, High Impact
V1-rated high impact styreneAll information provided by LTL Color Compounders, Inc.
Copyright © lookpolymers.com All Rights Reserved