Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 2180 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 15.0 MPa
>= 2180 psi
ISO 527
Murtfeldt Material ”S”® 1000 Black Antistatic Polyethylene, Conductive
Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio..
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 1000 - REG PE Colored
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 1000 - REG PE Multicoloured coarse
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 1000 PE-UHMW, Colored
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 1000 PE-UHMW, UV - stabilized
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Tensile Strength, Yield 15.0 MPa
2180 psi
ISO 527
Polimeri Europa Flexirene® MR 50 U Linear Low Density Polyethylene
Flexirene MR 50 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 U are characterized by optimum rigidity...
Tensile Strength, Yield 15.0 MPa
2180 psi
ASTM D412
Precision Polymer Engineering Z75L Hydrogenated NBR Compound
Peroxide Cured, Hydrogenated Nitrile Rubber, 75-85 °IRHD. Low acrylonitrile content (ACN = 17%).Applications: Specially compounded for service in low-temperature applications. High strength and ex..
Tensile Strength, Yield 15.0 MPa
2180 psi
ISO 527
Premix Thermoplastics PRE-ELEC® ESD 6600 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6000 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6000 has b..
Tensile Strength, Yield 15.0 MPa
2180 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DBP32EI PC
LNP* Lubricomp* DBP32EI is a compound based on Polycarbonate resin containing 15% PTFE/Silicone and 10% Glass Bead. Added features of this material include: Internally Lubricated.
Tensile Strength, Yield 15.0 - 18.0 MPa

@Thickness 2.00 mm
2180 - 2610 psi

@Thickness 0.0787 in
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)
Solef® 21510 PVDF copolymer has medium viscosity and is suitable for extrusion and for solution processing in lithium batteries applications.Features: Copolymer; Good Flexibility; Medium Viscosit..
Tensile Strength, Yield 15.0 MPa
2180 psi
ISO 527
Styrolution Styrolux BX6400 SBC
Styrolux BX6400 is a developmental styrene butadiene copolymer (SBC) of high clarity and ultimate toughness used mainly in sheet and film extrusion and thermoforming applications. It is specifically..
Tensile Strength, Yield 15.0 MPa
2180 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SIM 4515 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Tensile Strength, Yield 15.0 MPa
2180 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SSH 6009 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Good Flexibility Uses: Cable Jacketing; Wire and Cable Applications Wire Types: ST1; ST2; Type 9; Class 1/3; YM3; YM5 Agency Ratings: BS 6746; IEC 60502; JIS 672..
Tensile Strength, Yield 15.0 MPa
2180 psi
Trelleborg R350 Natural Rubber Polyisoprene
All information provided by Trelleborg
Tensile Strength, Yield 15.0 MPa
2180 psi
ASTM D638
Trelleborg Horda Cable E7355-A4 Strippable Semiconductive Shielding
E7355-A4 is a silane crosslinkable, strippable semiconductive compound for medium voltage cables.E7355-A4 meets the requirements as below, when optimal processing, extrusion and crosslinking procedu..
Tensile Strength, Yield 15.0 MPa
2180 psi
Trelleborg I644 Antiabrasive SBR Rubber
Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like..
Tensile Strength, Yield 15.0 MPa

@Strain 300 %
2180 psi

@Strain 300 %
ISO 527-1/-2
Covestro Desmopan® 3385A Polyurethane
Extrusion- and injection molding gradegood wear resistanceshort cycle timeshigh melt stabilityApplicationhard - soft systemsHosesnon-reinforcedProfilesInjection molded engineering partsPreprocessing..
Tensile Strength, Yield 15.0 MPa

@Strain 300 %
2180 psi

@Strain 300 %
ISO 527-1/-2
Covestro Desmopan® 3485A Polyurethane
Extrusion- and injection molding gradesuitable for extrusion blow moldingwith release agenthigh melt stabilityApplicationBellowsInjection molded engineering partsPreprocessingMax. Water content
Tensile Strength, Yield 15.0 MPa
2180 psi
ISO 527-1/-2
DSM Arnitel® UM552 Polyether Ester Elastomer (European Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 15.0 MPa
2180 psi
ISO 527-2/50
ExxonMobil Exxtral™ CMN 303 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for high heat ageing resistance for automotive interior trim applications such as instrument panels.Availability: Africa & Mi..
Tensile Strength, Yield 15.0 MPa
2180 psi
ISO 527-2/50
ExxonMobil Exxtral™ H1025W Performance Polyolefin
Product Description: A polyolefin injection molding compound designed with good flow, cold temperature impact resistance, low CLTE, weatherable mold-in-color and also suitable for painted automotive..
Tensile Strength, Yield 15.0 MPa
2180 psi
ISO 527-1/2
CTC SunPro® SP 200 TF 3033 Polypropylene Copolymer, 33% Talc Filled
SunPro® SP 200 TF 3033 is a 33% talc filled polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Application: VW TL 52660 MD 03Data ..
Tensile Strength, Yield 15.0 MPa
2180 psi
50 mm/min
Arkema Group Pebax® MV 1041 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) hardness 60 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....)ISO data provided ..
Tensile Strength, Yield 15.0 MPa
2180 psi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0437C10L Calcium Reinforced
Tensile Strength, Yield 15.0 MPa

@Strain 50.0 %
2180 psi

@Strain 50.0 %
50 mm/min
Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11-P,EHL,16-001High flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High burst pressure and impact strength..
Tensile Strength, Yield 15.0 MPa
2180 psi
ASTM D-638
Axiall 163 Moldings & Extrusions Flexible PVC
60°C rated, high flow, electrical molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 15.0 MPa
2180 psi
ASTM D638
NOVA Chemicals Sclair® 94D1 HDPE Extrusion Resin &nbsp;(discontinued **)
Features: Excellent processability, high stretchability, excellent strength.Applications: Package nettings for produce, Christmas tree wrap and turkey overwrap.Data provided by the manufacturer.
Tensile Strength, Yield 15.0 MPa
2180 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR DBPH-50
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 15.0 - 18.0 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
2180 - 2610 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type IV, 50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF) &nbsp;(Unverified Data**)
Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers.
Tensile Strength, Yield 15.0 MPa
2180 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Solvay Engineered Polymers DEXFLEX® 930 TPO &nbsp;(discontinued **)
Description: DEXFLEX® 930 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact propert..
Copyright © lookpolymers.com All Rights Reserved