| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
|
Ineos Nova Zyntar® F7120 Developmental Flame Retardant Polystyrene
(discontinued **)
Features: High flow for thin wall partsGood balance of physical propertiesUL94 V-0 @ 1.5 mm for black color Good aesthetics for injection molding Applications:Large television cabinetsConsumer elect..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3210 psi | |
|
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 6 PHR Varox DBPH-50
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM D638 |
|
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 18% Plasticizer
(discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
|
LyondellBasell Petrothene® KR92717 High Density Polyethylene
ApplicationsPETROTHENE KR 92717 is a high molecular weight, high density polyethylene-based compound designed for use in spacer cable insulation and cable jacketing applications. This black compoun..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | Type 1 Specimen, Rate: 2"/min; ASTM D638 |
|
Global GPP-2000 Polypropylene Impact Copolymer, Cold Temperature Impact Resistant, Nucleated
Information provided by Global Polymers Corporation.
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
|
Spartech PP7110 Talc Filled High Impact Copolymer
Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
|
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2"/min; ASTM D638 |
|
A. Schulman LP544-01 High-Density Copolymer Polyethylene
DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
|
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2"/min; ASTM D638 |
|
A. Schulman LP544-01 High-Density Copolymer Polyethylene
DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
|
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2 in/min; ASTM D638 |
|
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2"/min; ASTM D638 |
|
A. Schulman LP544-01 High-Density Copolymer Polyethylene
DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2"/min; ASTM D638 |
|
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | |
|
Zylog Hipolyene® 8501 T6 B Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
|
Total HDPE 7194 High Density Polyethylene, Specialty Extrusion Resin
Medium molecular weightNarrow molecular weight distributionDesigned for high speed orientationUSP Class VI compliantApplications:MonofilamentSlit tapeWoven and knitted fabricsSpecialty filmsInformat..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2" (50mm) per min.; ASTM D638 |
|
Formosa Plastics Formolene® 2520A Injection Molding Polypropylene
Medium Impact CopolymerApplications: Closures, Housewares, and Small Appliance ApplicationsFormolene 2520A is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2"/min; ASTM D638 |
|
A. Schulman LP544-01 High-Density Copolymer Polyethylene
DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM D638 |
|
Eastman Tenite Propionate 371A2R30012 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | ISO 527-1/2 |
|
CTC X-PRO CTC PP 2040 Polypropylene Copolymer
X-PRO PP 2040 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | ISO 527-2/1A/50 |
|
ExxonMobil HDPE HMA 018 High Density Polyethylene Resin
Product Description: HMA 018 is an easy flow HDPE grade, characterized by high gloss and dimensional stability. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabili..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
|
Entec Hyrene® PS-HI 3/4 High Impact Polystyrene
Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3210 psi | Molded property |
|
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2027A Polyethylene resin is a higher density polymer for cast film applications with improved stiffness. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2(a) for food contact appli..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
|
Asahi Kasei Thermylene® P-20TC-0736 20% Talc Filled, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3210 psi | Type IV, 510 mm/min; ASTM D638 |
|
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx92FRD Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2"/min; ASTM D638 |
|
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2"/min; ASTM D638 |
|
A. Schulman LP544-01 High-Density Copolymer Polyethylene
DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
|
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
|
Borealis Low Sulfur™ LE0595 Crosslinkable Semiconductive Compound for Shielding of Power Cables
Low Sulphur LE0595 is designed for use as a conductor and bonded insulation shield for medium and high voltage cables. LE0594 is a peroxide crosslinkable compound and is specifically intended to me..
|
|||
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2" (50mm) per min, Type IV; ASTM D638 |
|
Formosa Plastics Formolene® HP4000 Pipe HDPE
High Density Hexene Copolymer Formolene® HP4000 is a high performance copolymer that is designed for the most demanding requirements of non pressure pipe applications. It has good long-term hoop st..
|
|||