| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 16.7 - 17.2 MPa | 2420 - 2490 psi | ASTM D1708 |
| Polimersan Plastics POLITEF® (PTFE) with 60% Bronze As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
| Tensile Strength, Yield | 16.7 MPa | 2420 psi | ASTM D412 |
| Precision Polymer Engineering V60D Fluoroelastomer Compound Fluoroelastomer Rubber, 55-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet Aerospace Specifications DTD5612A and DTD5543B Grade 60.Applications: Mouldings which are re.. |
|||
| Tensile Strength, Yield | 16.7 - 17.2 MPa | 2420 - 2490 psi | ASTM D1708 |
| Polimersan Plastics POLITEF® (PTFE) with 60% Bronze As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
| Tensile Strength, Yield | 16.7 MPa @Thickness 3.20 mm |
2420 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
| LG Chemical LUPOL HI4352L PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9003-07-0, 26221-73-8 and 14807-96-6Inform.. |
|||
| Tensile Strength, Yield | 16.7 MPa @Thickness 3.20 mm |
2420 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
| LG Chemical LUPOL MC4352 PP+Rubber+MF Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, Scratch resistance, Good Weatherability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9.. |
|||
| Tensile Strength, Yield | 16.7 MPa | 2420 psi | ASTM D412 |
| Teknor Apex Flexalloy® 3500-75 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
| Tensile Strength, Yield | 16.7 MPa | 2420 psi | ASTM D412 |
| Teknor Apex ELEXAR® EL 8451 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
| Tensile Strength, Yield | 16.7 MPa | 2420 psi | 9.8 in/min; ASTM D638 |
| Teknor Apex Sinvicomp SFE 4500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Hose; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
| Tensile Strength, Yield | 16.7 MPa | 2420 psi | 9.8 in/min; ASTM D638 |
| Teknor Apex Sinvicomp SFE 5000 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Hose; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
| Tensile Strength, Yield | 16.7 MPa | 2420 psi | 9.8 in/min; ASTM D638 |
| Teknor Apex Sinvicomp SIM 4029 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
| Tensile Strength, Yield | 16.7 MPa | 2420 psi | 20 in/min; ASTM D638 |
| Teknor Apex Sinvicomp SMG 5000 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Toys Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
| Tensile Strength, Yield | 16.7 MPa | 2420 psi | |
| Zylog Hipolyene® 1048 X1 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
| Tensile Strength, Yield | 16.7 MPa | 2420 psi | |
| Zylog Hipolyene® GM BP 11 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
| Tensile Strength, Yield | 16.7 MPa | 2420 psi | at 300% elongation; ASTM D412 |
| Lubrizol Estane® R190A Thermoplastic Polyurethane Type: Estane® R190A is a Shore 93A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi.. |
|||
| Tensile Strength, Yield | 16.7 MPa | 2420 psi | 9.8 in/min; ASTM D638 |
| Teknor Apex Sinvicomp SIH 5569 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Stiffness Uses: Electronic Insulation; Wire and Cable Applications Wire Types: A; B; YI4; YI5 Agency Ratings: IEC 60502; VDE 0207 Forms: Pellets Processing .. |
|||