| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 15.0 - 20.0 MPa | 2180 - 2900 psi | 50 mm/min; ISO/R 527 |
|
Okulen® 1000 - REG PE Colored
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Tensile Strength, Yield | 15.0 - 20.0 MPa | 2180 - 2900 psi | 50 mm/min; ISO/R 527 |
|
Okulen® 1000 - REG PE Multicoloured coarse
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Tensile Strength, Yield | 15.0 - 20.0 MPa | 2180 - 2900 psi | 50 mm/min; ISO/R 527 |
|
Okulen® 1000 PE-UHMW, AST
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Tensile Strength, Yield | 15.0 - 20.0 MPa | 2180 - 2900 psi | 50 mm/min; ISO/R 527 |
|
Okulen® 1000 PE-UHMW, Black
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Tensile Strength, Yield | 15.0 - 20.0 MPa | 2180 - 2900 psi | 50 mm/min; ISO/R 527 |
|
Okulen® 1000 PE-UHMW, Colored
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Tensile Strength, Yield | 15.0 - 20.0 MPa | 2180 - 2900 psi | 50 mm/min; ISO/R 527 |
|
Okulen® 1000 PE-UHMW, Conductive
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Tensile Strength, Yield | 15.0 - 20.0 MPa | 2180 - 2900 psi | 50 mm/min; ISO/R 527 |
|
Okulen® 1000 PE-UHMW, MoS2 -Moly-
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Tensile Strength, Yield | 15.0 - 20.0 MPa | 2180 - 2900 psi | 50 mm/min; ISO/R 527 |
|
Okulen® 1000 PE-UHMW, UV - stabilized
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Tensile Strength, Yield | 15.0 - 20.0 MPa | 2180 - 2900 psi | 50 mm/min; ISO/R 527 |
|
Okulen® 500 - REG PE Colored
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
|
|||
| Tensile Strength, Yield | 10.0 - 20.0 MPa | 1450 - 2900 psi | 50 mm/min; ISO/R 527 |
|
Okulen® 500 - REG PE Multicoloured coarse
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
|
|||
| Tensile Strength, Yield | 10.0 - 20.0 MPa | 1450 - 2900 psi | 50 mm/min; ISO/R 527 |
|
Okulen® 500 - REG PE Multicoloured fine
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
|
|||
| Tensile Strength, Yield | 15.0 - 20.0 MPa | 2180 - 2900 psi | 50 mm/min; ISO/R 527 |
|
Okulen® 500 PE-HMW, AST
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
|
|||
| Tensile Strength, Yield | 15.0 - 20.0 MPa | 2180 - 2900 psi | 50 mm/min; ISO/R 527 |
|
Okulen® 1000 - REG PE Multicoloured fine
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Tensile Strength, Yield | 14.0 - 20.0 MPa | 2030 - 2900 psi | Average value: 16.6 MPa Grade Count:5 |
|
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma..
|
|||
| Tensile Strength, Yield | 17.0 - 20.0 MPa | 2470 - 2900 psi | ASTM D638M |
|
DSM Somos® 9420 Epoxy Resin for Stereolithography
DescriptionDSM Somos® 9420 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance and a wid..
|
|||