| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield |
2.07
MPa <br>@Strain 100 %
|
300
psi <br>@Strain 100 %
|
across flow; ASTM D412 |
|
ExxonMobil Santoprene® 8291-65TB Thermoplastic Rubber
(discontinued **)
Description: A colorable thermoplastic elastomer which bonds to adhesive/epoxy spin-finished polyester or standard nylon fibers for closed-braid hose and woven-substrate products. With bonds strong..
|
|||
| Tensile Strength, Yield | 2.07 - 53.8 MPa | 300 - 7800 psi | Average value: 18.4 MPa Grade Count:7 |
|
Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Thermoplastic Polyurethane Blend". Each property range of values reported is minimum and m..
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | No units listed, assumed to be psi. |
|
COR12V Cork/Neoprene Rubber Sheet
Description: Harvested every 9-12 years from the cork oak tree, cork is able to rebound from compression with extrusion. Applications include: stoppers, soundproofing, flooring, gaskets, and many ot..
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | @ 50% Elongation; ASTM D1414 |
|
Greene Tweed CHEMRAZ® 514 Perfluoroelastomer
Greene Tweed’s Chemraz® 514, a perfluoroelastomer, is a white specialty compound, perfect for applications where contamination from carbon black must be prevented. Chemraz 514 offers a Shor..
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | @50% Elongation; ASTM D1414 |
|
Greene Tweed CHEMRAZ® 534 Perfluoroelastomer
Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r..
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | at 100%; ASTM D412 |
|
Multibase Multi-Flex® A 7206 E TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
|
|||
| Tensile Strength, Yield | >= 2.07 MPa | >= 300 psi | Stress at Elongation M100; ASTM D412 Method A |
|
Seals Eastern 7202 Nitrile Rubber
Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc.
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | 100%; ASTM D412 |
|
Teknor Apex APEX® 1519-39 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMForms-PelletsFeatures- Good flexibility Information provided by Teknor Apex Company
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | 100%; ASTM D412 |
|
Teknor Apex Flexalloy® 3500-40 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te..
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | 100%; ASTM D412 |
|
Teknor Apex Flexalloy® 9100-35 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather..
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | ASTM D412 |
|
Teknor Apex MONPRENE® MP 1900 Thermoplastic Elastomer
Information provided by Teknor Apex Company
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | ASTM D412 |
|
Teknor Apex MONPRENE® MP 2720 Thermoplastic Elastomer
Information provided by Teknor Apex Company
|
|||
| Tensile Strength, Yield |
2.07
MPa <br>@Strain 300 %
|
300
psi <br>@Strain 300 %
|
ASTM D412 |
|
Teknor Apex Monprene® MP 3005L3 Thermoplastic Elastomer
Notes: Translucent Features: Good Chemical and Oil Resistance; Tough; Good Melt StrengthInformation Provided by Teknor Apex
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | 100%; ASTM D412 |
|
Teknor Apex APEX® 3210-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
|
|||
| Tensile Strength, Yield |
2.07
MPa <br>@Strain 300 %
|
300
psi <br>@Strain 300 %
|
ASTM D412 |
|
Teknor Apex Monprene® MP 1544 Thermoplastic Elastomer
Notes: Translucent Features: Good Chemical and Oil ResistanceInformation Provided by Teknor Apex
|
|||
| Tensile Strength, Yield |
2.07
MPa <br>@Strain 300 %
|
300
psi <br>@Strain 300 %
|
ASTM D412 |
|
Teknor Apex Monprene® MP 1644 Thermoplastic Elastomer
Notes: Clear Features: High Flow; High Coefficient of FrictionInformation Provided by Teknor Apex
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | |
|
Master Bond Mastersil 700 One Component High Temperature Resistant Silicon
Master Bond MasterSil 700 is a ready-to-use, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. It remains flexible and..
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | |
|
Master Bond Mastersil 701 One Component, Room Temperature Curing Silicone Elastomer
Master Bond Master Sil 701 is a ready-to-use, one component, high performance silicone elastomer compound for bonding, and sealing protective coatings and formed-in-place gaskets. It cures at ambien..
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | at 150% Elongation, maximum |
|
Dow Corning SILASTIC® LCS-755 SILICONE RUBBER
55 Durometer, translucent, low compression set, uncatalysed Silicone Rubber Base suitable for molding.Information provided by Dow Corning
|
|||
| Tensile Strength, Yield |
2.07
MPa <br>@Strain 300 %
|
300
psi <br>@Strain 300 %
|
ASTM D412 |
|
Teknor Apex Monprene® MP 1579 Thermoplastic Elastomer
Notes: Translucent Features: Good Chemical and Oil Resistance; Tough; Good Melt StrengthInformation Provided by Teknor Apex
|
|||
| Tensile Strength, Yield |
2.07
MPa <br>@Strain 300 %
|
300
psi <br>@Strain 300 %
|
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
|
PolyOne Synprene® IT 086LFR Thermoplastic Elastomer - SBC
(discontinued **)
Description/Features:Flame RetardantMulti-Purpose Thermoplastic ElastomerApplications:General PurposeInteriorProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Co..
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | TM R050-36 |
|
Resinlab® EP1200 Black Casting Resin
Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re..
|
|||
| Tensile Strength, Yield | 2.07 - 53.1 MPa | 300 - 7700 psi | Average value: 13.6 MPa Grade Count:449 |
|
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | at 100%; ASTM D412 |
|
R70-058 Styrene-based Biomedical Elastomer |
|||
| Tensile Strength, Yield | 2.07 - 75.0 MPa | 300 - 10900 psi | Average value: 27.9 MPa Grade Count:100 |
|
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | at 100%; ASTM D412 |
|
MF-5040 Polyurethane-based Biomedical Elastomer |
|||
| Tensile Strength, Yield |
2.07
MPa <br>@Strain 300 %
|
300
psi <br>@Strain 300 %
|
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
|
PolyOne Synprene® RT-3740 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding..
|
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | at 100%; ASTM D412 |
|
MF-5001 Polyurethane-based Biomedical Elastomer |
|||
| Tensile Strength, Yield | 2.07 MPa | 300 psi | at 100%; ASTM D412 |
|
MF-5041 Polyurethane-based Biomedical Elastomer |
|||