Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 3770 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
ISO 527-2
Total Lacqrene® 4240(EU) High Impact Polystyrene  (discontinued **)
LACQRENE® 4240 is a high heat resistance, high impact polystyrene for the extrusion industry. Good mechanical and thermal properties leads to the production of thermoformed articles of good rigidi..
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638M
DSM Somos® WaterClear® 10120 Epoxy Resin for Stereolithography  (discontinued **)
DescriptionDSM Somos® 10120 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us..
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Flint Hills AP5520-HA Polypropylene Impact Copolymer
Features: Nucleated, good processability, anti-stat and good mold release.Applications: Injection molding: large parts, containers, closuresInformation Provided by Flint Hills Resources
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Flint Hills AP6106-HS Impact Copolymer Polypropylene
High impact copolymer, UL certified, and FDA compliant. Features: Heat stabilizedApplications: Injection molding: child protection systems, appliance components, consumer durables, and automotive in..
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Ineos Styrenics Avantra® 585K Rubber Modified Polystyrene
Avantra® 585K is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical impact strength. Although Avantra® 585K can be processed by any method applicable..
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
IRPC Polimaxx Polene 3325M Polypropylene Random Copolymer
CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD SEALABLE CONTAINS SLIP AND ANTIBLOCK ADDITIVES APPLICATIONS: CAST FILM EXTRUSION CPP FILM FOR LAMINATE , CPP FILM FOR PACKAGINGS
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Global PP-2300-SC Polypropylene Block Copolymer
Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-thin walled parts, electrical appliancesInformation provided by Global Polymers Corporation.
Tensile Strength, Yield >= 26.0 MPa
>= 3770 psi
Sibur 21030-PM1 Polypropylene with Low Haze
For production of three-layer PE/PP film, for production of sheets for cups and thin casting. It is allowed for contact with food products.
Tensile Strength, Yield 26.0 MPa
3770 psi
50 mm/min; ISO 527-1/-2
Styrolution Polystyrol 495 F GR 2 PS
Description: Polystyrol 495 F is a high impact polystyrene with a good heat resistance and high stiffness.Applications: Consumer electronics; TV-front and back; chassis for VCR and CD player. Househ..
Tensile Strength, Yield 26.0 MPa
3770 psi
ISO 527
Styrolution PS 495F HIPS
Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection..
Tensile Strength, Yield 26.0 MPa
3770 psi
ISO 527-1/-2
Styrolution Styrolux® 684 D SBC
Description: Styrolux® 684 D is a clear styrene-butadiene copolymer (SBC) used in injection molding for parts with enhanced toughness as well as in sheet and film extrusion and blow molding. Part..
Tensile Strength, Yield 26.0 MPa
3770 psi
50mm/min; ISO 527-2
Borealis BE375MO Polypropylene Copolymer
BE375MO is a heterophasic copolymer. This grade is characterized by optimum combination of high impact strength and stiffness. This grade is formulated for an excellent antistatic performance. Elect..
Tensile Strength, Yield 26.0 MPa
3770 psi
50mm/min; ISO 527-2
Borealis BF330MO Polypropylene Copolymer
BF330MO is a heterophasic copolymer. This polymer is characterized by an optimum combination of high stiffness, high impact strength and good flow properties. This grade is designed for high-speed i..
Tensile Strength, Yield 26.0 MPa
3770 psi
50mm/min; ISO 527-2
Borealis BH374MO Polypropylene Copolymer
BH374MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. Products molded with this grade exhibi..
Tensile Strength, Yield 26.0 MPa
3770 psi
50mm/min; ISO 527-2
Borealis MG9621S Polyethylene
MG9621S is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of..
Tensile Strength, Yield 26.0 MPa
3770 psi
At 50 mm/min; ISO 527-2
Borealis Xmod™ BE677AI High Crystalline Polypropylene Copolymer
Xmod BE677AI is a UV-stabilized HCPP intended for injection molding of automotive interior and appliance parts. Xmod BE677AI has an excellent balance between impact strength and stiffness as well ..
Tensile Strength, Yield 26.0 MPa
3770 psi
24 min.; ASTM D638
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene
DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman.
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Tipco Tipcolene® FPT 20 FR VO LTHA - UL94-V0 Flame Retardant, 20% Talc Polypropylene Homopolymer, Long Term Heat Stability
20% Talc Reinforced PP Homopolymer with Long Term Heat StabilityApplications: Electrical & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., Ind..
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
A. Schulman POLYFORT™ PP 3045
Information provided by A. Schulman.
Tensile Strength, Yield 26.0 MPa
3770 psi
50mm/min; ISO 527-2
Borealis RB206MO Polypropylene Random Copolymer
RB206MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade also ..
Tensile Strength, Yield 26.0 MPa
3770 psi
ISO 527-2
Tisan TISOPLEN® 20% Calcite Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Tensile Strength, Yield 26.0 MPa
3770 psi
ISO 527-2
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Tensile Strength, Yield 26.0 MPa
3770 psi
Total Xsene® XS10 B HDPE, pipe, injection molding
FINATHENE® XS10 B is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS10 B is a high performance black compound speci..
Tensile Strength, Yield 26.0 MPa

@Strain 300 %
3770 psi

@Strain 300 %
ISO 527-1/-2
Covestro Desmopan® DP 3354D Polyurethane
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Tensile Strength, Yield 26.0 MPa
3770 psi
BASF Novolen® 2309 L Polypropylene
Cast film and thermoformed partsData was collected by ISO methods and provided by BASF.
Tensile Strength, Yield 26.0 MPa
3770 psi
BASF Polystyrol® 476 L Impact Grade Polystyrene (Europe)
Normal flowing, high-impact grade. When extruded it is often mixed with PS 165 H.Data was collected by ISO methods and provided by BASF.
Tensile Strength, Yield 26.0 MPa
3770 psi
50 mm/min
Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical..
Tensile Strength, Yield 26.0 MPa

@Strain 0.200 %,
Temperature 1204 °C
3770 psi

@Strain 0.200 %,
Temperature 2199 °F
Haynes 230® alloy, cold rolled and 1232°C solution annealed sheet
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Copyright © lookpolymers.com All Rights Reserved