Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Multibase Multi-Pro® 1505 R Polypropylene
Glass Fiber Reinforced, 15% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Multibase Multi-Pro® 4010 M Polypropylene
Mica Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses:Pump PartsInformation provided by Multibase
Tensile Strength, Yield 40.7 MPa
5900 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion LR620 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Polymer Resources ABS-FR Flame Retardant ABS
Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch..
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized
Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and..
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Polimeri Europa SINKRAL B532 ABS, Very High Impact  (discontinued **)
Very high impact; injection/extrusion grade.Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Ravago Manufacturing Americas Hylac® GP48 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Techmer ES HiFill FR® ABS FR
Availability: North AmericaForms: PelletsFeatures: Flame RetardantTPCI# 1039121Information provided by TP Composites, Inc.
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Techmer ES HiFill FR® ABS FR BK
Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackTPCI# 9224121Information provided by TP Composites, Inc.
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Techmer ES HiFill FR® ABS FR UV
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc.
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Techmer ES HiFill FR® ABS FR UV BK
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant and Good UV ResistanceUL File Number: E157318Appearance: BlackTPCI# 9224121Information provided by TP Compos..
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Techmer ES HiFill FR® ABS FR V2 BK
Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Spartech Royalite R522 PVC Alloy Aircraft Grade Sheet
Description: Aircraft Grade SheetInformation provided by Spartech.
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Spartech Royalite R60 PVC/Acrylic Aircraft Grade Sheet
Description: Aircraft Grade SheetInformation provided by Spartech.
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Spartech Royalite R66 PVC/Acrylic Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Techmer ES HiFill FR® PA6 E FR
Availability: North AmericaForms: PelletsFeatures: Flame Retardant Processing Method: ExtrusionInformation provided by TP Composites, Inc.
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Eastman Tenite 285E3720005 Butyrate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Tensile Strength, Yield 40.7 MPa
5900 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS 7600B (ELG)
Description: Blow Molding Grade, Extra High Impact, Low GlossInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 40.7 MPa
5900 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS/PC 7901
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 40.7 MPa
5900 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers Centrex® 810 Injection Molding Grade
Centrex 810 resin is a soft-flow, high-gloss, and medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and ..
Tensile Strength, Yield 40.7 MPa
5900 psi
chs 50 mm/min; tangent; ASTM D638
Diamond Polymers NPP30-2000HC Homopolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Eastman Tenite Propionate 358A4000018 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 8%. Weight loss on heating = 0.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D-638
Axiall 9246 Rigid PVC, Molding
Georgia Gulf 9246 is a high impact compound suitable for food packaging.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D-638
Axiall 7407 Rigid PVC, Extrusion
Georgia Gulf 7407 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D-638
Axiall 7765 Rigid PVC, Extrusion
Georgia Gulf 7765 is a general-purpose indoor rigid PVC profile extrusion compound designed for applications requiring the following properties. 7765 carries an NSF standard 51 listing (for food zo..
Tensile Strength, Yield 40.7 - 181 MPa
5900 - 26200 psi
Average value: 114 MPa Grade Count:35
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Tensile Strength, Yield 40.7 - 121 MPa
5900 - 17500 psi
Average value: 62.8 MPa Grade Count:27
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Polimeri Europa SINKRAL G523 ABS, High Impact  (discontinued **)
High impact; good flow; high gloss.Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Spartech Royalite R60-LS (R61) PVC/Acrylic Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.