| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Geloy XTWM200 ASA
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | 50 mm/min |
|
Polimeri Europa KOBLEND HI 41 F1 PBT+PC, Impact Grade
(discontinued **)
Symbol according to ISO 1043/1: PBT+PC-HI Similar to KOBLEND HI 41 with improved fluidity. Main application fields: bumpers Unfilled. Suitable for Injection Molding. Supplied as pellets.ISO data..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
|
Global PC/ABS-1003 General Purpose Polycarbonate/ABS Alloy
Information provided by Global Polymers Corporation.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Asia Pacific)
LNP Lubricomp* KL004 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* Fu..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527 type 1 A |
|
Solvay TECHNYL® A 246M PA66, DRY
Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copolymer
LNP* LUBRICOMP* KL004L is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer (Asia Pacific)
LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT
LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS (Asia Pacific)
LNP LUBRICOMP ZL003 is a compound based on PPE+PS Blend resin containing PTFE. Added features of this material include:internally Lubricated. Also known as LUBRICOMP ZL-4030
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRILOY R2000A PA 66
LNP LUBRILOY* R2000A is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER
Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant...
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Europe-Africa-Middle East)
Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant...
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | Type I, 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Asia Pacific)
Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527-2 |
|
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided ..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP WZ002 PBT
LNP* THERMOCOMP* WZ002 is a compound based on PBT resin containing 10% Milled Glass.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER (Europe-Africa-Middle East)
Polyester+PC alloy. Diffusion Effect. Color package may affect performance.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527 |
|
A. Schulman FORMION™ FI 233 15% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 233 is an injection molding grade, 15% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. A..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527 |
|
Eastman DuraStar DS1110UVI Polymer, Natural
Durastar DS1110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527 |
|
Eastman DuraStar MN621 Polymer, Natural
Durastar Polymer MN621 was developed for the medical device industry and contains a mold release It processes easily and requires minimal drying time. It has superior toughness, high clarity and goo..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | 50 mm/min |
|
Arkema Group Rilsan® AECV T8L Nylon 12, Cable Sheathing Grade (Dry)
Designation ISO 1874-PA12,KHL,16-010Extrusion grade for the sheathing of wires and cables. Available colors: black, blue, orange and white. Reinforced light and heat stabilizing agents. Anti-termite..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
|
Aclo Accutech Polypropylene Homopolymer HP0339G15M15CL Glass/Mineral Reinforced Coupled |
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
|
Ashley Polymers Ashlene® P114 PBT Polyester
A high impact polyester with low shrinkage.Data provided by the manufacturer
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East)
Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS
Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen..
|
|||
| Tensile Strength, Yield | 47.0 - 90.0 MPa | 6820 - 13100 psi | Average value: 62.4 MPa Grade Count:26 |
|
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
|
|||