Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific)
PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication.
Tensile Strength, Yield 51.0 MPa
7400 psi
50 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Europe-Africa-Middle East)
High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Polymer Resources PC-IM3 Polycarbonate, Impact Modified, High Flow
Polycarbonate, Impact Modified, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Polymer Resources TP-M30 Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced Warpage
Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Ineos Nova 1210 High Heat Crystal Polystyrene  (discontinued **)
High heat resistance, High molecular weight, optimum performance in extruded foamApplications: Meat and poultry trays, Egg cartons, Food packagingExposure to gamma radiation in the 2.02-6.06 megarad..
Tensile Strength, Yield 51.0 MPa

@Temperature 23.0 °C
7400 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® ST800HSL BK152 Nylon 66  (Unverified Data**)
Zytel® ST800HSL BK152 is a heat stabilized Super Tough black polyamide 66 resin. It offers outstanding impact resistance, high productivity and laser markability.Information provided by DuPont
Tensile Strength, Yield 51.0 MPa

@Thickness 3.20 mm
7400 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOY GP5006AF PC/ABS, Flame Retardant
Description: Injection Molding, PC/ABS, Flame RetardantApplication: Electric and Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chem..
Tensile Strength, Yield 51.0 MPa

@Thickness 3.20 mm
7400 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
LG Chemical XR440 ABS, Low Emission High Heat ABS
Feature: Injection Molding Grade, Low Emission High Heat ABSApplication: Automotives Interior housingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer
LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant.
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated.
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer (Asia Pacific)
LNP Lubricomp* KL004U is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* F..
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer (Asia Pacific)
LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
Tensile Strength, Yield 51.0 MPa
7400 psi
ISO 527
SABIC Innovative Plastics LNP Lubriloy D2000XXH PC
LNP LUBRILOY* D2000XXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated, Healthcare.This data was supplied..
Tensile Strength, Yield 51.0 MPa
7400 psi
Type I, 50 mm/min; ASTM D 638
SABIC Innovative Plastics Valox® 312 PBT
Unreinforced, For compounding only (not for injection molding), FDA (21 CFR 177.1660) compliant. Medium viscosity.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength, Yield 51.0 MPa
7400 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics Xenoy® 1103 PBT+PC
AUTOMOTIVE. Unreinforced, impact modified PBT+PC alloy. Excellent low temperature impact and chemical resistance. Range gray, black colors.
Tensile Strength, Yield 51.0 MPa
7400 psi
Type I, 50 mm/min; ASTM D 638
SABIC Innovative Plastics Xenoy® X6125 PBT+PC
Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength, Yield 51.0 MPa
7400 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-LOY 9X07438 ASA+PC
LNP* STAT-LOY* 9X07438 is a compound based on Polycarbonate/ASA containing Proprietary Filler(s). Added features of this grade include: Antistatic, Colorable, Weatherable.
Tensile Strength, Yield 51.0 MPa
7400 psi
ISO 527
Styrolution Novodur® H802 ABS
Novodur H802 is a high heat injection molding grade with high stiffness, especially suitable for being painted.Information provided by Styrolution
Tensile Strength, Yield 51.0 MPa
7400 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SF-0950 MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 51.0 MPa
7400 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP TF006 PU
LNP THERMOCOMP TF006 is a compound based on Polyurethane containing 30% Glass Fiber.
Tensile Strength, Yield 51.0 MPa
7400 psi
50 mm/min; ISO 527
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific)
PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance.
Tensile Strength, Yield 51.0 MPa
7400 psi
ISO 527-2
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin
Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can ..
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Total PSC 535 Polystyrene
Polystyrene 535 is a high heat crystal polystyrene designed for injection molding, extrusion and blow molding. The material demonstrates excellent strength and good temperature resistance. The varie..
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Tipco Tipcolene® SEB 300 M - 30% Chemically Coupled Glass Fibers & Mineral Polypropylene Homopolymer
30% Mineral + Glass Reinforced, PP Homopolymer for Automobile Engine PartsApplications: Automotive Engine PartsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries..
Tensile Strength, Yield 51.0 MPa
7400 psi
50 mm/min
Arkema Group Rilsan® MB 3000 Nylon 11, Sheathing Grade (Dry)
Designation ISO 1874-PA11,MF,12-010Polyvalent rigid grade for injection molding and sheathing of cables. Available color: natural. Flame retardant agent, halogen free. Fire-resistant. Easy to be pro..
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Ashley Polymers Ashlene® D926 Nylon 12
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. Also availabl..
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Ineos Nova 1220 High Heat Crystal Polystyrene  (discontinued **)
Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r..
Tensile Strength, Yield 51.0 MPa

@Thickness 3.20 mm
7400 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
LG Chemical MA201 ABS, Low Gloss
Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical