| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | ASTM D638 |
|
NYCOA 715C PA 6
plasticized, high viscosity extrusion grade for monofilament weed eater, fishing lineInformation provided by NYCOA, Inc.
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Asia Pacific)
High flow PC+ABS.
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS
PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components.
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Asia Pacific)
PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components.
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer
Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char..
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in..
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Asia Pacific)
Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb..
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer
Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are..
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Asia Pacific)
Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch..
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXE1162T PC Copolymer (Europe-Africa-Middle East)
Lexan* FXE1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c..
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer
Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil..
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer (Asia Pacific)
Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in ""Energy"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color pac..
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® FXC1200E PC+ABS (Asia Pacific)
Visual Fx PC/ABS for strong fluorescent bright colors with good flow, impact and heat resistance characteristics. Consumer electronic and appliance applications uses.
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color.
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was suppli..
|
|||
| Tensile Strength, Yield |
57.0
MPa @Temperature 23.0 °C |
8270
psi @Temperature 73.4 °F |
50mm/min; ISO 527-2/1A/50 |
|
SYNTHOS Forsan® 393 Acrylonitrile Butadiene Styrene (ABS)
High heat resistance, high gloss.Applications: Electrotechnics, lighting equipment, automotiveHousehold appliances, electric switches, lamps, car interior parts, etc.Synthos was formerly known as Ka..
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | ISO 527 |
|
SABIC Innovative Plastics LNP STAT-KON DD000P PC (Asia Pacific)
LNP* Stat-kon* DD000P is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Exceptional Processing.
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | ASTM D 638 |
|
SABIC Innovative Plastics LNP Stat-kon DX92440 PC
LNP STAT-KON* DX92440 is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied..
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER
PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER (Asia Pacific)
PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP STAT-LOY Cycoloy_CA6200 PC+ABS
PRELIMINARY DATA. LNP* Stat-loy* Cycoloy_CA6200 compound is a Non-ECO flame retardant, anti-static PC+ABS for ESD management.
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | SABIC - Japan Method |
|
SABIC Innovative Plastics Valox® V3504 PBT (Asia Pacific)
VALOX EXVX0197 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | ISO 527-1/-2 |
|
DuPont Performance Polymers Crastin® S600F20 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 BK851 is an unreinforced lubricated medium viscosity black polybutylene terephthalate resin for injection molding.Information..
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | ASTM D638 |
|
E-Polymers Tekaloy® G70FR , Flame Retardant, Un-Reinforced PC/ABS Alloy
Flame Retardant, Impact ResistanceInformation provided by E-Polymers Co. Ltd.
|
|||
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | ASTM D638 |
|
E-Polymers Tekaloy® G70A2 Impact Resistance, Easy Molding PC/ABS Alloy
Impact Resistance, Easy MoldingInformation provided by E-Polymers Co. Ltd.
|
|||