Polymer Property : Tensile Strength, Yield = 6000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging 2121 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging 2160 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87549 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Strength, Yield 41.4 MPa
6000 psi
51 mm/min; ASTM D638
PolyOne Trilliant™ HC X THC 1101 Natural Copolyester
Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Polymer Resources NY66-IM2-LM Nylon, Preliminary Data Sheet, Low Flexural Modulus, High Impact (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Tensile Strength, Yield 41.4 MPa
6000 psi
5.1 mm/min; ASTM D638
PolyOne Edgetek® X TR2-10TA/000 NATURAL Copolyester
The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea..
Tensile Strength, Yield 41.4 MPa
6000 psi
51 mm/min; ASTM D638
PolyOne Edgetek® XT X XT 1001 Natural Copolyester
Edgetek™ XT high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Edget..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
M. Holland Company AB103LG ABS Acrylonitrile Butadiene Styrene
Medium flowMedium impact resistanceGood stiffnessInformation provided by M. Holland
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Techmer ES HiFill® PA11 GB30 HS 30% Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformation provided by ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Spartech Korad® SP-9071 FR/ABS Flame Retardant Sheet
Description: Flame Retardant SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Spartech Panel Pro ABS UV-Resistant Embossed Sheet Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Spartech SP-9010 General Purpose ABS Sheet
Description: ABS SheetInformation provided by Spartech.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Star Plastics ABSLG3030 Molding Grade ABS, Low Gloss
Information provided by Star Plastics, Inc.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Techmer ES Plastiblend® ABS/PBT 1000
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
Tensile Strength, Yield 41.4 MPa

@Thickness 3.20 mm
6000 psi

@Thickness 0.126 in
Injection Molded; ASTM D638
Styron MAGNUMâ„¢ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 342 EZ ABS resin is a medium impact, high flow, low gloss resin often used in automotive applications. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, imp..
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 51 mm/min; ASTM D638
Styron MAGNUMâ„¢ 347 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM Data
Styron Magnumâ„¢ 800 ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM Data
Styron Magnumâ„¢ 941 ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Techmer ES HiFill® PA6 0254 B2 Barium Sulfate Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific Gravity and AntistaticAdditive: AntistaticInformation provided by TP Composites, Inc.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Techmer ES Luriblend® POM CO TL20 LE Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%) and Silicone LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction, Low Extractables and CopolymerUL File Number: E..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Clariant Renol BR4014BK ABS, High Gloss, Black
Data provided by Clariant Masterbatches
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Axiall SP-7107 Rigid PVC, Molding
Georgia Gulf SP-7107 is a general purpose, electrical grade rigid vinyl injection molding compound characterized by excellent flow, heat stability, color hold and surface appearance. This makes it ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Axiall UV-6670 Rigid PVC, Molding
Georgia Gulf UV-6670 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Axiall 7055 Rigid PVC, Extrusion
Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: WeatherabilityChemicalDurabilityEase of ProcessingToughnessInformat..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Axiall 7555 Rigid PVC, Extrusion, Natural
Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Axiall 8302 Rigid PVC, Extrusion & Molding
Georgia Gulf 8302 is a clear rigid PVC pellet compound suited for applications where transparency is important in a high sunlight environment. It can be used for exterior transparent profiles such ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Axiall 9113J Clear 13, 9113J Clear 61 Rigid PVC, Molding, Clear 13, Clear 61
Georgia Gulf 9113J Clear 13 and 9113J Clear 61 are used for a variety of packages including charcoal lighter fluid, toiletries and household chemicals. They have excellent impact strength and conta..
Tensile Strength, Yield 41.4 - 70.0 MPa
6000 - 10200 psi
Average value: 52.8 MPa Grade Count:13
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Eastman Tenite 360A4861301 Propionate Clear, Trsp  (discontinued **)
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM Data
Styron Magnum™ 9020 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB..