Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.0 MPa
6090 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics Cycolac® FR23 ABS
Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated.
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D638
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East)
LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D638
SABIC Innovative Plastics LNP FARADEX AS003 ABS
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding...
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D638
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Europe-Africa-Middle East)
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Tensile Strength, Yield 42.0 MPa
6090 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC
LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing 10% Glass Beads and 15% PTFE. Added features of this material include: Internally Lubricated.
Tensile Strength, Yield 42.0 MPa
6090 psi
50 mm/min
Polimeri Europa SINKRAL B633/E ABS, Impact & Heat Stabilized Grade  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,105-04-25-20 High impact extrusion grade with excellent stiffness, good processability and high thermal stabili..
Tensile Strength, Yield 42.0 MPa
6090 psi
50 mm/min
Arkema Group Oroglas® HFI-10 Acrylic, Impact Grade  (discontinued **)
OROGLAS HFI-10 is an impact grade that in addition to its superior impact resistance provides an improvement in flow which contribute to improve molding behavior and reduce cycle time.Key features :..
Tensile Strength, Yield 42.0 MPa
6090 psi
ISO R527
Fainplast Compounds RKI 0822 Rigid PVC, Antishock Injection Molding Lead Free
Technical items
Tensile Strength, Yield 42.0 MPa
6090 psi
50 mm/min; ISO 527
LG Chemical LI-913 ASA, Injection Molding, High Impact
Information Provided by LG Chem
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM-D638
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade
Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)...
Tensile Strength, Yield 42.0 MPa
6090 psi
50 mm/min; ISO 527-1,-2
Ineos ABS Lustran® M210TF ABS Pellets
Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo..
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC (Asia Pacific)
LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated.
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D 638
SABIC Innovative Plastics LNP Lubricomp DP003F PC
LNP LUBRICOMP* DP003F is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the..
Tensile Strength, Yield 42.0 MPa
6090 psi
ISO 527
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50
Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin..
Tensile Strength, Yield 42.0 MPa
6090 psi
ISO 527 type 1 A
Solvay TECHNYL® A 246M PA66, DRY
Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN..
Tensile Strength, Yield 42.0 MPa
6090 psi
ISO 527
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA
LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer
LNP THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing 20% Milled Glass.
Tensile Strength, Yield 42.0 MPa
6090 psi
2 in/min; ASTM Test
Styrolution Terlux® 2812 TR MABS
Terlux 2812 TR is a transparent grade of MABS for injection molding with high flowability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Tensile Strength, Yield 42.0 MPa
6090 psi
SABIC - Japan Method
SABIC Innovative Plastics Noryl INT1000 PPE+HIPS (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Strength, Yield 42.0 MPa
6090 psi
SABIC - Japan Method
SABIC Innovative Plastics Noryl EBN9003 PPE+HIPS (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Strength, Yield 42.0 MPa
6090 psi
ISO 527
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
Tensile Strength, Yield 42.0 MPa
6090 psi
ISO 527
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D638
UBE UBESTA® 3030UFX1 Rigid Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
Tensile Strength, Yield 42.0 MPa
6090 psi
50 mm/min
Arkema Group Orgalloy® RS 60E10TL Nylon 6 Alloy, Rigid Grade (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie..
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D638
Aclo Accucomp ABS ABS846HL High Flow Medium Impact Grade
Tensile Strength, Yield 42.0 MPa
6090 psi
50 mm/min
Arkema Group Rilsan® BESN TL Nylon 11, Rigid Tubing Grade (Conditioned)
Designation ISO 1874-PA11,EHL,22-010Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Good chemical resistanc..
Tensile Strength, Yield 42.0 MPa
6090 psi
50 mm/min
Arkema Group Rilsan® BUM 30 Nylon 11, 30% Glass Bead Filled (Dry)
Designation ISO 1874-PA11,M,18-020,GB30Rigid grade with glass beads (30%) filler for injection molding. Available colors: black and natural. Additive free.Outstanding isotropic properties. High comp..
Tensile Strength, Yield 42.0 MPa
6090 psi
50mm/min; ASTM D638
3M Dyneon™ PVDF 6008/0001 Polyvinylidene Fluoride
Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an..
Tensile Strength, Yield 42.0 MPa
6090 psi
Fainplast Compounds RE 220 Rigid PVC, Extrusion
Various profiles
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D638
BP Amoco Accpro® 9961 Enhanced Polypropylene  (discontinued **)
Suggested fabrication methods: Injection moldingFeatures: NucleatedTypical applications: CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection..