| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 62.1 MPa | 9010 psi | Type I, 5.1 mm/min; ASTM D638 |
|
PolyOne Gravi-Tech™ GRV-NY-112-W-NAT Polyamide 6 (Nylon 6)
Information provided by PolyOne
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
|
Oxford Polymers PC 912 Unfilled Polycarbonate for Injection and Extrusion Molding
Unfilled Polycarbonate for Injection and Extrusion MoldingInformation provided by Oxford Polymers.
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
|
Polymer Resources PC-GP3-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release
Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp..
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
|
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release
Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
|
Polymer Resources PPX-GP5 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 270F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Tensile Strength, Yield |
62.1
MPa @Thickness 3.17 mm |
9010
psi @Thickness 0.125 in |
ASTM D638 |
|
PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Tensile Strength, Yield |
62.1
MPa @Thickness 3.17 mm |
9010
psi @Thickness 0.125 in |
ASTM D638 |
|
PTS Tristar® PC-10R-(VE) 12 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Tensile Strength, Yield | 62.1 - 125 MPa | 9000 - 18100 psi | Average value: 99.3 MPa Grade Count:63 |
|
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
|
Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
|
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam..
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
|
Polymer Resources PC-UV3-D-[color]-1 Polycarbonate, UV-stabilized, High Flow with Mold Release
Polycarbonate, UV-stabilized, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
|
|||
| Tensile Strength, Yield |
62.1
MPa @Thickness 3.17 mm |
9010
psi @Thickness 0.125 in |
ASTM D638 |
|
PTS Tristar® PC-10FR-(16) 16 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Tensile Strength, Yield |
62.1
MPa @Thickness 3.17 mm |
9010
psi @Thickness 0.125 in |
ASTM D638 |
|
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Tensile Strength, Yield |
62.1
MPa @Thickness 3.17 mm |
9010
psi @Thickness 0.125 in |
ASTM D638 |
|
PTS Tristar® PC-10R-(V) 10 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Tensile Strength, Yield |
62.1
MPa @Thickness 3.17 mm |
9010
psi @Thickness 0.125 in |
ASTM D638 |
|
PTS Tristar® PC-10R-(V18) 18 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
|
Global PC-1415-R General Purpose Polycarbonate
Information provided by Global Polymers Corporation.
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
|
Global PC-1418 General Purpose Polycarbonate
Information provided by Global Polymers Corporation.
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
|
Global PC-FR0 UL Recognized 94V-0 Polycarbonate
Information provided by Global Polymers Corporation.
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | 2.0 in/min; ASTM D638 |
|
LTL Color Compounds ColorFast® PC100 Polycarbonate
10 melt standard injection molding gradeAll information provided by LTL Color Compounders, Inc.
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
|
Techmer ES HiFill® PA6/6 GF8 IM4 HS L 8% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 8% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Compo..
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
|
Star Plastics PC743 Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9010 psi | ASTM Data |
|
Styron CALIBREâ„¢ 2060 10 Polycarbonate, Sterilization Grade
CALIBRE® 2060 series resins are designed for those applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clari..
|
|||
| Tensile Strength, Yield |
62.1
MPa @Thickness 3.17 mm |
9010
psi @Thickness 0.125 in |
|
|
Samyang Trirex® PC-3025IR 10 MFI Clear Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9010 psi | 50 mm/min; ASTM D638 |
|
Styron CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate Resin
Overview: CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to hi..
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D882 |
|
Specialty Coating Systems Parylene D Poly (P-Xylylene) Coating
Parylene D is a polymer of para-xylylene modified by the substitution of chlorine atoms for two of the aromatic hydrogen atoms. Parylene D is similar in properties to Parylene C with the added abili..
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
|
Techmer ES HiFill® PPSU A1 0200 B LE
Availability: North AmericaForms: PelletsFeatures: High Density and Low ExtractablesAppearance: OpaqueInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
|
Westlake Plastics Zelux® M Machine Grade Polycarbonate
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ISO 527 |
|
A. Schulman SCHULAMID® 6 GB30 30% Glass Bead Reinforced Nylon 6
Information provided by A. Schulman.
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D-638 |
|
Axiall ProTherm® 4529 CPVC Rigid PVC, Molding
Georgia Gulf ProTherm® 4529 CPVC is a pelletized injection molding compound designed for large fittings. Typical applications are in potable water and chemical transfer systems especially where hi..
|
|||
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | 2.0 in/min; ASTM D638 |
|
LTL Color Compounds ColorFast® FRPC400 Polycarbonate, Flame-Retarded
Flame-retarded V0, high impact injection molding polycarbonateAll information provided by LTL Color Compounders, Inc.
|
|||