| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycolac® MG38F ABS (Asia Pacific)
Very high impact ABS. Toughness/rigidity. FDA compliant.
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycolac® MG38U ABS
High impact ABS. UL 746C f1 listed. Toughness/rigidity. Good fatigue resistance.
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific)
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Geloy XTWM206 ASA (Asia Pacific)
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Asia Pacific regio..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | |
|
Reliance Industries Polypropylene - 30% glass fiber filled
Information provided by Reliance Industries
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
|
Ineos ABS Lustran® Ultra 2337 General Purpose, Superhigh-Gloss
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | 50 mm/min |
|
Polimeri Europa SINKRAL A22V ABS
(discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-09-25 Very high flow grade for fast cycle injection moulding. Particularly recommended for the domestic ..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO R527 |
|
Fainplast Compounds RST 0413 Rigid PVC, Extrusion Lead Free
Transparent antishock profiles
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527 |
|
GEHR Plastics POM-10PE Acetal Copolymer
Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC
LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing 20% PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | SABIC - Japan Method |
|
SABIC Innovative Plastics NORYL SE100P PPE+HIPS (Asia Pacific) |
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP SG004 PA12 (Europe-Africa-Middle East)
LNP* LUBRICOMP* SG004 is a compound based on PA 12 resin containing Graphite. Added features include: Internally Lubricated.
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP Lubricomp WL0049XF PBT
LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant.This data was suppl..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527 |
|
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS
LNP* STAT-LOY* AF306 is a compound based on ABS resin containing 30% Glass Fiber. Added feature of this material is: Antistatic.
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | 50mm/min; ISO 527 |
|
Styrolution Terblend® N NM-19 ABS/PA6 (Dry)
Terblend N NM-19 is a UV stabilized ABS/PA6 blend combining very high impact strength, even at low temperatures with an excellent processability and surface appearance.Information provided by STYROL..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527-1/-2 |
|
Styrolution Terblend® N NM-19 XP Beige 38163 ABS+PA (Dry)
Description: Terblend® N NM-19 XP is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures with an outstanding processability and excellent surface appearanc..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL EM6100 PPE+PS
PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
|
UBE UBESTA® 3024NUX Short Cycle Time Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
|
Eastman Tritan MX731 Copolyester
Eastman Tritan Copolyester MX731 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX731 is a high flow medical grade of Eastman Tritan that has viscosity re..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
|
Eastman Tritan TX1001 Copolyester
Eastman Tritan TX1001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX1001 contains a mold release derived from vegetable based sources. Its most outstanding fe..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
|
Eastman Tritan TX1500HF Copolyester
Eastman Tritan TX1500HF is a high flow grade of Eastman Tritan. Eastman Tritan TX1500HF has viscosity reductions of 40-50% relative to Eastman Tritan copolyester TX1000. Other outstanding features..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527-1/-2 |
|
DuPont Performance Polymers Delrin® 100STE NC010 Acetal (POM)
(Unverified Data**)
Super Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100STE NC010 (formerly DE20590) is a high-viscosity super-toughened acetal homopolymer with very low VOC emissions. P..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | |
|
Fainplast Compounds R 220 Rigid PVC, Extrusion
Rolling shutters
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | |
|
Fainplast Compounds R 220/R Rigid PVC, Extrusion
Shiny rolling shutters
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | 50mm/min; ISO 527 |
|
BASF Ultramid® 8202C HS PA6 (Conditioned)
Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | 2 in/min; ASTM Test |
|
BASF Ultramid® 8202CQ PA6 (Conditioned)
Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527-2 |
|
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
|
Ineos Nova 3511 General Purpose Crystal Polystyrene
(discontinued **)
Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure..
|
|||
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics GELOY CR7500 ASA