| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | Type I, 51 mm/min; ASTM D638 |
|
PolyOne Geon™ Vinyl Packaging 161J-4-DD Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | Type I, 5.1 mm/min; ASTM D638 |
|
PolyOne LubriOne™ AT-000/15T Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D638 |
|
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow
Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D638 |
|
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow
Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM Data |
|
Americas Styrenics Styron® 666D Polystyrene
(discontinued **)
STYRON® 666D general purpose polystyrene resin is used in injection molding applications, particularly for medical, pharmaceutical and food uses. It offers excellent clarity, intermediate flow char..
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D638 |
|
M. Holland Company SA500 Styrene Acrylonitrile
High clarityGood processabilityHigh stiffnessApplications: Color concentratesCompounding
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D638 |
|
Techmer ES HiFill® ABS LG GF10 UV BK 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAdditive: UV StabilizerFeatures: Good UV Resistance and Low GlassAppearance: BlackInform..
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D638 |
|
Techmer ES HiFill® PA6 0390 BK
Availability: North AmericaForms: PelletsFeatures: High Specific GravityAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D638 |
|
Techmer ES HiFill® PA6/6 0249 B Nylon 66
Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D 638 |
|
Styrolution PS 3190/3191 GPPS
Low residual styrene monomer contentGood balance of flow and set-up propertiesInformation provided by Styrolution
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM Data |
|
Styron Magnumâ„¢ 780HP ABS, High Heat, High Impact
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM Data |
|
Styron Magnumâ„¢ 9555 ABS, High Impact
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D638 |
|
Techmer ES HiFill® PA6 0425
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D638 |
|
Techmer ES HiFill® TPU/E 0140
Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM Data |
|
Styron Magnumâ„¢ 344HP ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D638 |
|
Westlake Plastics Dielux® PTFE filled Acetal Copolymer
Dielux PTFE filled acetal copolymer is an outstanding bearing and wear material for use in both wet and dry environments. It is frequently used in place of traditional metal and plastic bearing mat..
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | chs 2 in/min; ASTM D638 |
|
Diamond Polymers ABS 3501
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | chs 2 in/min; ASTM D638 |
|
Diamond Polymers ABS 3501 Natural 1002 ESCR Injection Molding Grade, Environmental Stress Crack Resistant
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | chs 2 in/min; ASTM D638 |
|
Diamond Polymers ABS 3502
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D638 |
|
Clariant PA131 Nylon 66, Highly Impact Modified
Data provided by Clariant Masterbatches
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D638 |
|
Clariant Renol PA133GN-109 Nylon 66, High Impact, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D-638 |
|
Axiall CL-6400 Rigid PVC, Molding
Georgia Gulf CL-6400 is a high flow clear PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information p..
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D-638 |
|
Axiall Suprel® SVA 9812 Rigid PVC, Extrusion
Georgia Gulf Suprel® SVA 9812 Alloy is an extrusion grade thermoplastic designed for sheet or profile applications requiring high impact resistance. Key features of Suprel 9812 alloy are flame ret..
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D-638 |
|
Axiall Tuf-Stif 2802 Rigid PVC, Extrusion
Georgia Gulf Tuf-Stif 2802 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit..
|
|||
| Tensile Strength, Yield |
44.8
MPa @Thickness 3.17 mm |
6500
psi @Thickness 0.125 in |
Type I; ASTM D638 |
|
Calsak CS-72L General Purpose ABS Resin
Product Characteristics:High Impact, High GlossInjection molding grade
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D-638 |
|
Axiall 7045 Rigid PVC, Extrusion
Georgia Gulf 7045 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityDimen..
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
|
PolyOne Edgetek® AT-30GB/000 Acetal-Copolymer, Glass Bead Filled
(discontinued **)
Description/Features:Glass Bead FilledInformation provided by PolyOne Corporation.
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D-638 |
|
Axiall 3240 Rigid PVC, Extrusion
Georgia Gulf 3240 is a special purpose rigid powder blend PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChe..
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D-638 |
|
Axiall 9017J Clear 06 Rigid PVC, Molding, Clear
Georgia Gulf 9017J Clear 06 is for food packaging and personal care applications requiring optimum taste and odor properties. The compound contains an ultraviolet light stabilizer, which protects l..
|
|||
| Tensile Strength, Yield | 44.8 MPa | 6500 psi | ASTM D-638 |
|
Axiall 2512 Rigid PVC, Extrusion