| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Geloy XTWM200 ASA
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific)
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | Type I, 5.1 mm/min; ASTM D638 |
|
PolyOne Geon™ Vinyl Dry Blend E7009 Polyvinyl Chloride, Rigid (PVC, Rigid)
Recommended for whites and light pastel colors only. Not to be used for darker colors.Physical properties based on Geon E7009 white 1024 lot# UTCX 57572Information provided by PolyOne
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Cycoloy® CM8622 PC+ABS (Europe-Africa-Middle East)
CYCOLOY* CM8622 is a high heat PC/ABS blend offering high modulus, low CTE and good
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
|
Ineos Nova 1531 High Heat Crystal Polystyrene
(discontinued **)
High flow and high heat resistance, Excellent clarityApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optical p..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
|
Ineos Nova 1504 High Heat Crystal Polystyrene
Good balance of flow, strength and set up properties, Blue edge effect, USP Class VIApplications: Consumer electronics, Housewares, Cosmetic packagingExposure to gamma radiation in the 2.02-6.06 meg..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Europe-Africa-Middle East)
LNP* LUBRICOMP* KL004 is a compound based on Acetal Copolymer containing PTFE. Added features include Internally Lubricated.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer
LNP LUBRICOMP* KL004U is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, UV Stabilized.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer (Asia Pacific)
LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT
LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
|
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS (Asia Pacific)
LNP LUBRICOMP ZL003 is a compound based on PPE+PS Blend resin containing PTFE. Added features of this material include:internally Lubricated. Also known as LUBRICOMP ZL-4030
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | Type I, 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | 50 mm/min; ISO 527-1/-2 |
|
Styrolution Luran® S 776 S Colored ASA
Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527 |
|
Styrolution Novodur® 4115 ABS
Novodur Ultra 4115 is a PC modified high heat injection molding grade. It provides good heat resistance combined with high impact strength.Information provided by Styrolution
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527 |
|
Styrolution Novodur® H605 ABS
Novodur H605 is a high heat injection molding grade with enhanced flowability and reduced emission.Information provided by Styrolution
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527-2 |
|
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527-2 |
|
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided ..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP WZ002 PBT
LNP* THERMOCOMP* WZ002 is a compound based on PBT resin containing 10% Milled Glass.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | Elastic Limit |
|
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy
Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
|
Eastman DuraStar MN610 Polymer, Natural
Durastar MN610 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN610 has very ..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527 |
|
Eastman DuraStar MN611 Polymer, Natural
Durastar Polymer MN611 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
|
Eastman Eastar BR001 Copolyester
Eastar BR001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
|
Eastman Eastar DN001HF Copolyester
Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN001HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
|
Ashley Polymers Ashlene® P114WO PBT Polyester
A high impact polyester with low shrinkage, flame retardant.Data provided by the manufacturer
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | SABIC - Japan Method |
|
SABIC Innovative Plastics NORYL 115 PPE+HIPS (Asia Pacific)
PPE+PS, 115 oC HDT
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East)
Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen..
|
|||
| Tensile Strength, Yield | 47.0 - 90.0 MPa | 6820 - 13100 psi | Average value: 62.4 MPa Grade Count:26 |
|
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
|
SABIC Innovative Plastics LNP STAT-KON ME003S PP
LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized.
|
|||
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ISO 527 |
|
SABIC Innovative Plastics LNP STAT-KON ME003S PP
LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized.
|
|||