Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 - 85.0 MPa
10900 - 12300 psi
Type 1B, 50mm/min; ISO 527-1/2:1993
Nylacast Aquanyl Nylon 612 Copolymer
Aquanyl is a copolymer of Nylon 6 and Nylon 12 produced via the anionic polymerization process using the monomer's Caprolactam and Laurinlactam. It has reduced water absorption, improved stability a..
Tensile Strength, Yield 75.0 - 85.0 MPa
10900 - 12300 psi
Type 1B, 50mm/min; ISO 527-1/2:1993
Nylacast Nylube Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant)
This supreme wear resistant grade contains a combined liquid/solid lubricant system, which allows for a coefficient of friction as low as 0.08. The material has outstanding Pressure-Velocity capabil..
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO 527
SABIC Innovative Plastics LNP COLORCOMP R1000S PA 66
LNP COLORCOMP* R1000S is an unfilled Nylon 66. Added features of this material is: Heat Stabilized.
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO 527
SABIC Innovative Plastics LNP COLORCOMP R1000SU PA 66
LNP COLORCOMP* R1000SU is an unfilled Nylon 66 resin. Added features include: Heat Stabilized, UV Stabilized.
Tensile Strength, Yield 75.0 - 275 MPa
<br>@Temperature -50.0 - 250 °C
10900 - 39900 psi
<br>@Temperature -58.0 - 482 °F
Average value: 169 MPa Grade Count:1
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
Tensile Strength, Yield >= 75.0 MPa
>= 10900 psi
MetalTek Bearium® B-4 Bearing Bronze
Exceptional frictional properties as a result of uniformly dispersed microstructure constituents.Applications: Turbine thrust bearings, centrifuge bushings, shaft sleeves, and other severe duty, mis..
Tensile Strength, Yield 75.0 MPa
10900 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RL002 PA 66
LNP LUBRICOMP* RL002 is a compound based on Nylon 66 resin containing 10% PTFE. Added features of this material include: Wear Resistant.
Tensile Strength, Yield 75.0 MPa
10900 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East)
VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries.
Tensile Strength, Yield 75.0 MPa
10900 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp DFZ22E PC
LNP* Thermocomp* DFZ22E is a compound based on Polycarbonate with Glass and Milled Fiber. Characteristics of this products is Easy Molding.This data was supplied by SABIC-IP for the Americas region..
Tensile Strength, Yield 75.0 MPa
10900 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL HH180 PPE+PS (Asia Pacific)
Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365.
Tensile Strength, Yield 75.0 MPa
10900 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL N1150 PPE+PS
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO 527
SABIC Innovative Plastics NORYL N300X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications.
Tensile Strength, Yield 75.0 MPa
10900 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp RB003 PA 66 (Europe-Africa-Middle East)
15% glass beads filled polyamide 66 injection moulding resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Strength, Yield 75.0 MPa
10900 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Asia Pacific)
PPE+PS blend. 10% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including wate..
Tensile Strength, Yield 75.0 MPa
10900 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO 527-2
Tisan TISLAMID® 6 30% Mineral Reinforced Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Tensile Strength, Yield >= 75.0 MPa
>= 10900 psi
ASTM-D638
Polyram PlusTek RA102 Nylon 6.6, General Purpose
General purpose polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO 527
Polyram RamLloy PFS302G14 ASA/PBT Alloy, 14% Glass Fiber
14% Glass fiber reinforced ASA/PBT alloy for injection molding applications.Information provided by Polyram.
Tensile Strength, Yield 75.0 MPa
10900 psi
50 mm/min; ISO 527-1,-2
Covestro Makrolon® FR 7087 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
Tensile Strength, Yield 75.0 MPa
10900 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® EB 50 H PA6
Product description: Grilon EB 50 H is a high viscosity, unreinforced, heat stabilized PA6 extrusion blow mounding grade. Grilon EB 50 H has the following important properties: High melt strengthImp..
Tensile Strength, Yield 75.0 MPa
10900 psi
50 mm/min; ISO 527
CP-Polymer-Technik Wellamid® 6600/506 HWCP Nylon 66, Impact Modified, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Tensile Strength, Yield 75.0 MPa
10900 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® TR 55 PA12/MACMI
Product description: Grilamid TR 55 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 55 natural offers outstanding properties..
Tensile Strength, Yield 75.0 MPa
10900 psi
ASTM D638
E-Polymers TEKAMID® TB120L Lubricated PA6, DAM
LubricatedInformation provided by E-Polymers Co. Ltd.
Tensile Strength, Yield 75.0 MPa
10900 psi
50mm/min; ISO 527-2
BASF Ultrason S 2010 PSU
Ultrason S 2010 is an unreinforced, medium viscosity standard injection molding PSU grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..
Tensile Strength, Yield 75.0 MPa
10900 psi
dry; ISO 527
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored
Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac..
Tensile Strength, Yield 75.0 MPa
10900 psi
ASTM value at 50 mm/min.
BASF Capron® 8362 HS Impact Modified, 34% Mineral-Filled Nylon 6 (Dry) &nbsp;(discontinued **)
Capron 8362 HS is a 34% glass reinforced, impact modified, heat stabilized nylon6 injection molding compound exhibiting a high level of toughness in combination with excellent processability and sur..
Tensile Strength, Yield 75.0 MPa
10900 psi
Radici Radilon® A 35E 990 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Tensile Strength, Yield 75.0 MPa
10900 psi
50mm/min; ISO 527
BASF Ultrason S 6010 PSU
Ultrason S 6010 is an unreinforced, high molecular weight injection-molding and extrusion grade with excellent chemical resistance (stress crack resistance) and good solubility in typical solvents (..
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO 527
Polyram RamTough PZ304G2 Polycarbonate, 10% Glass Fiber
10% glass fiber reinforced polycarbonate for injection molding applications.Information provided by Polyram.
Tensile Strength, Yield 75.0 MPa
<br>@Strain 0.200 %,<br> Temperature 1100 °C
10900 psi
<br>@Strain 0.200 %,<br> Temperature 2010 °F
Special Metals UDIMET® alloy L-605 Co-Cr-W-Ni Alloy
UDIMET® alloy L-605 (UNS R30605) is a solid solution strengthened cobalt-chromium-tungsten-nickel alloy with excellent high-temperature strength and excellent oxidation resistance to 2000°F (1093°..